Preparation method of blue-and-white Nixing ceramic
The invention discloses a preparation method of blue-and-white Nixing ceramic. The preparation method comprises the following step: (1) preparing a blank: preparing the blank from the following raw materials in parts by weight: 45 to 55 parts of east mud, 40 to 50 parts of west mud, 7 to 9 parts of kaolin, 1 to 3 parts of bentonite, 1 to 3 parts of feldspar, 4 to 6 parts of quartz and 2 to 4 parts of talcum; (2) forming the blank; (3) trimming the blank; (4) drying the blank; (5) decorating the blank: drawing a pattern and writing characters on the blank by using cobalt blue material; (6) firing. According to the preparation method, by adjusting the formula of the blue-and-white paint, a color development temprature range of the blue-and-white paint is consistent with a firing temperature range of the Nixing ceramic blank; a stepped continuous temperature rising and reducing method is used for firing, so that the blue-and-white decorative Nixing ceramic is realized and a practical value of the Nixing ceramic is increased; the formula is reasonable, the production cost is low and the firing rate is high.
Preparation method of blue-and-white Nixing ceramic
The invention discloses a preparation method of blue-and-white Nixing ceramic. The preparation method comprises the following step: (1) preparing a blank: preparing the blank from the following raw materials in parts by weight: 45 to 55 parts of east mud, 40 to 50 parts of west mud, 7 to 9 parts of kaolin, 1 to 3 parts of bentonite, 1 to 3 parts of feldspar, 4 to 6 parts of quartz and 2 to 4 parts of talcum; (2) forming the blank; (3) trimming the blank; (4) drying the blank; (5) decorating the blank: drawing a pattern and writing characters on the blank by using cobalt blue material; (6) firing. According to the preparation method, by adjusting the formula of the blue-and-white paint, a color development temprature range of the blue-and-white paint is consistent with a firing temperature range of the Nixing ceramic blank; a stepped continuous temperature rising and reducing method is used for firing, so that the blue-and-white decorative Nixing ceramic is realized and a practical value of the Nixing ceramic is increased; the formula is reasonable, the production cost is low and the firing rate is high.
Preparation method of blue-and-white Nixing ceramic
HUANG TAOMO (author)
2016-01-27
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Preparation method for novel nixing ceramic decorated with blue-and-white material
European Patent Office | 2016
|Preparation method for cobalt blue material decorative Nixing pottery
European Patent Office | 2016
|Novel combination method of cobalt blue material and Nixing ceramic
European Patent Office | 2016
|