Firing process and firing equipment of medium-temperature Longquan cyan glaze
The invention discloses a firing process and equipment of medium-temperature Longquan cyan glaze. The oxide comprises the following chemical components in percentage by weight: 62-66% of SiO2, 14-16%of Al2O3, 0.3-0.8% of MgO, 11-17% of CaO, 3-5% of K2O, 0.2-0.5% of Na2O, 0-0.25% of TiO2, 0.03-0.1% of MnO and 0.1-0.15% of Fe2O3. The firing process and firing equipment of medium-temperature Longquan cyan glaze are different from the prior art, the problem of chromatic aberration is likely to occur in the celadon glaze in large-batch production is solved, uniform and stable firing in the celadonglaze firing process can be guaranteed, celadon of various sizes can be subjected to efficient rotary firing protection, absolutely stable and safe uniform firing is guaranteed, meanwhile, inclined celadon can be effectively reset, and then high-quality firing is guaranteed.
本发明公开了一种中温龙泉青釉的烧制工艺及设备,其氧化物化学组成按重量百分比计为:62~66%SiO2,14~16%Al2O3,0.3~0.8%MgO,11~17%CaO,3~5%K2O,0.2~0.5%Na2O,0~0.25%TiO2,0.03~0.1%MnO,0.1~0.15%Fe2O3,此中温龙泉青釉的烧制工艺及其烧制设备,区别于现有技术,在解决了大批量生产过程中,其青釉易出现色差的难题的同时,能够保证青釉烧制过程中的均匀稳定烧制,能够对各尺寸青瓷进行高效的旋转烧制防护,保证绝对稳定安全的均匀烧制,且同时能够对倾斜的青瓷进行有效的复位,进而保证高质量烧制。
Firing process and firing equipment of medium-temperature Longquan cyan glaze
The invention discloses a firing process and equipment of medium-temperature Longquan cyan glaze. The oxide comprises the following chemical components in percentage by weight: 62-66% of SiO2, 14-16%of Al2O3, 0.3-0.8% of MgO, 11-17% of CaO, 3-5% of K2O, 0.2-0.5% of Na2O, 0-0.25% of TiO2, 0.03-0.1% of MnO and 0.1-0.15% of Fe2O3. The firing process and firing equipment of medium-temperature Longquan cyan glaze are different from the prior art, the problem of chromatic aberration is likely to occur in the celadon glaze in large-batch production is solved, uniform and stable firing in the celadonglaze firing process can be guaranteed, celadon of various sizes can be subjected to efficient rotary firing protection, absolutely stable and safe uniform firing is guaranteed, meanwhile, inclined celadon can be effectively reset, and then high-quality firing is guaranteed.
本发明公开了一种中温龙泉青釉的烧制工艺及设备,其氧化物化学组成按重量百分比计为:62~66%SiO2,14~16%Al2O3,0.3~0.8%MgO,11~17%CaO,3~5%K2O,0.2~0.5%Na2O,0~0.25%TiO2,0.03~0.1%MnO,0.1~0.15%Fe2O3,此中温龙泉青釉的烧制工艺及其烧制设备,区别于现有技术,在解决了大批量生产过程中,其青釉易出现色差的难题的同时,能够保证青釉烧制过程中的均匀稳定烧制,能够对各尺寸青瓷进行高效的旋转烧制防护,保证绝对稳定安全的均匀烧制,且同时能够对倾斜的青瓷进行有效的复位,进而保证高质量烧制。
Firing process and firing equipment of medium-temperature Longquan cyan glaze
一种中温龙泉青釉的烧制工艺及其烧制设备
LIN HUANYI (author) / DENG CHONG (author) / LIN SHAOSEN (author) / ZHOU JUNMIN (author) / YAO XIANLONG (author)
2020-06-19
Patent
Electronic Resource
Chinese
Glaze material for firing Longquan celadon thick glaze and firing process
European Patent Office | 2022
|Longquan Ge kiln hundredfold crackle glaze and firing process thereof
European Patent Office | 2020
|Archaistic grey glaze Longquan celadon and preparation process thereof
European Patent Office | 2024
|