Artificial stone and preparation method thereof
The invention relates to the technical field of artificial stones, in particular to an artificial stone and a preparation method thereof. The artificial stone comprises, by weight, 40-80 parts of potassium feldspar, 15-25 parts of pyroxene, 15-25 parts of quartz, 2.5 parts of a synthesis agent, wherein the main component of the potassium feldspar is SiO2, Al2O3, CaO and Fe2O3, the main component of the pyroxene is Al2O3, the main component of the quartz is SiO2, and the optimal weight ratio is as follows: 60 parts of the potassium feldspar, 20 parts of the pyroxene, 20 parts of the quartz and2.5 parts of the synthetic agent. According to the artificial stone and the preparation method thereof, the potassium feldspar, the pyroxene and the quartz are used for replacing a quartz stone or glass stone material, the optimal loose specific gravity is tested through multiple times of grain composition, and the specific gravity of the molded artificial stone is infinitely close to the specificgravity of natural granite. Moreover, the raw materials are available in many ways and are convenient and environment-friendly, so that the price of the main filler is lower, the production cost of the artificial granite can be greatly reduced, and environmental protection is facilitated.
本发明涉及人造石技术领域,具体为一种人造石及其制备方法。一种人造石,包括钾长石、辉石、石英、合成剂,其重量配比为:钾长石40‑80份、辉石15‑25份、石英15‑25份、合成剂2.5份,且钾长石的主要成分为SiO、AlO、CaO、FeO,辉石的主要成分为AlO,石英的主要成分为SiO,其最佳重量配比为:钾长石60份、辉石20份、石英20份、合成剂2.5份。该人造石及其制备方法,通过利用钾长石、辉石、石英来代替石英石或玻璃石材料,且在若干次颗粒级配,试验出最佳松散比重,成型后无限接近天然花岗石比重。而且原料获取途径多,且方便环保,让主填料的价格更便宜,能大大降低人造花岗石的生产成本的同时,也有利于环保。
Artificial stone and preparation method thereof
The invention relates to the technical field of artificial stones, in particular to an artificial stone and a preparation method thereof. The artificial stone comprises, by weight, 40-80 parts of potassium feldspar, 15-25 parts of pyroxene, 15-25 parts of quartz, 2.5 parts of a synthesis agent, wherein the main component of the potassium feldspar is SiO2, Al2O3, CaO and Fe2O3, the main component of the pyroxene is Al2O3, the main component of the quartz is SiO2, and the optimal weight ratio is as follows: 60 parts of the potassium feldspar, 20 parts of the pyroxene, 20 parts of the quartz and2.5 parts of the synthetic agent. According to the artificial stone and the preparation method thereof, the potassium feldspar, the pyroxene and the quartz are used for replacing a quartz stone or glass stone material, the optimal loose specific gravity is tested through multiple times of grain composition, and the specific gravity of the molded artificial stone is infinitely close to the specificgravity of natural granite. Moreover, the raw materials are available in many ways and are convenient and environment-friendly, so that the price of the main filler is lower, the production cost of the artificial granite can be greatly reduced, and environmental protection is facilitated.
本发明涉及人造石技术领域,具体为一种人造石及其制备方法。一种人造石,包括钾长石、辉石、石英、合成剂,其重量配比为:钾长石40‑80份、辉石15‑25份、石英15‑25份、合成剂2.5份,且钾长石的主要成分为SiO、AlO、CaO、FeO,辉石的主要成分为AlO,石英的主要成分为SiO,其最佳重量配比为:钾长石60份、辉石20份、石英20份、合成剂2.5份。该人造石及其制备方法,通过利用钾长石、辉石、石英来代替石英石或玻璃石材料,且在若干次颗粒级配,试验出最佳松散比重,成型后无限接近天然花岗石比重。而且原料获取途径多,且方便环保,让主填料的价格更便宜,能大大降低人造花岗石的生产成本的同时,也有利于环保。
Artificial stone and preparation method thereof
一种人造石及其制备方法