Microwave dielectric ceramic powder and preparation method and application thereof
The invention discloses microwave dielectric ceramic powder and a preparation method and application thereof. The microwave dielectric ceramic powder comprises ceramic powder prepared from the following raw materials in parts by weight: 35 to 45 parts of strontium carbonate, 15 to 25 parts of titanium oxide, 25 to 35 parts of lanthanum oxide, 5 to 15 parts of aluminum oxide, 0.1 to 0.2 part of cerium oxide and 0.008 to 0.02 part of manganese oxide. The microwave dielectric ceramic powder prepared by the method is a microwave dielectric material with a dielectric constant of 40, a high QxFo [ceramic quality factor] value and low loss, the electrical performance of microwave components such as a cavity filter can be significantly improved, especially the insertion loss of the filter is reduced, and a more stable temperature coefficient is obtained so that the influence on the filter due to use environment factors in actual use is reduced.
本发明公开了一种微波介质陶瓷粉及其制备方法、及其应用,微波介质陶瓷发包括以下原料按照重量份制备而成的陶瓷粉末:碳酸锶35‑45份、氧化钛15‑25份、氧化镧25‑35份、氧化铝5‑15份、氧化铈0.1‑0.2份、以及氧化锰0.008‑0.02份。本发明制备的微波介质陶瓷粉为介电常数40的高QxFo[陶瓷品质因素]值、低损耗的微波介质材料,能显著改善微波元器件如腔体滤波器的电性能,特别是降低滤波器的插入损耗,获得更稳定的温度系数,以减少滤波器在实际使用中因使用环境因素对滤波器所造成的影响。
Microwave dielectric ceramic powder and preparation method and application thereof
The invention discloses microwave dielectric ceramic powder and a preparation method and application thereof. The microwave dielectric ceramic powder comprises ceramic powder prepared from the following raw materials in parts by weight: 35 to 45 parts of strontium carbonate, 15 to 25 parts of titanium oxide, 25 to 35 parts of lanthanum oxide, 5 to 15 parts of aluminum oxide, 0.1 to 0.2 part of cerium oxide and 0.008 to 0.02 part of manganese oxide. The microwave dielectric ceramic powder prepared by the method is a microwave dielectric material with a dielectric constant of 40, a high QxFo [ceramic quality factor] value and low loss, the electrical performance of microwave components such as a cavity filter can be significantly improved, especially the insertion loss of the filter is reduced, and a more stable temperature coefficient is obtained so that the influence on the filter due to use environment factors in actual use is reduced.
本发明公开了一种微波介质陶瓷粉及其制备方法、及其应用,微波介质陶瓷发包括以下原料按照重量份制备而成的陶瓷粉末:碳酸锶35‑45份、氧化钛15‑25份、氧化镧25‑35份、氧化铝5‑15份、氧化铈0.1‑0.2份、以及氧化锰0.008‑0.02份。本发明制备的微波介质陶瓷粉为介电常数40的高QxFo[陶瓷品质因素]值、低损耗的微波介质材料,能显著改善微波元器件如腔体滤波器的电性能,特别是降低滤波器的插入损耗,获得更稳定的温度系数,以减少滤波器在实际使用中因使用环境因素对滤波器所造成的影响。
Microwave dielectric ceramic powder and preparation method and application thereof
一种微波介质陶瓷粉及其制备方法、及其应用
CHE HANSHUAI (author) / CHEN RONGDA (author) / CUI RONGJI (author)
2020-08-11
Patent
Electronic Resource
Chinese
European Patent Office | 2020
|European Patent Office | 2021
|European Patent Office | 2020
|Improved microwave dielectric ceramic powder and preparation method and application thereof
European Patent Office | 2020
|European Patent Office | 2021
|