The invention discloses an environment-friendly asphalt mixture and a preparation method thereof, and relates to the technical field of asphalt mixtures. The technical key points are as follows: the environment-friendly asphalt mixture comprises 50-80 parts of rock asphalt; 150 to 200 parts of matrix asphalt; 3-5 parts of plant asphalt; 90 to 140 parts of mineral powder; 500 to 700 parts of basaltaggregate; and 5-10 parts of an adhesive. The preparation method comprises the following steps: S1, putting the basalt aggregate into a drying barrel, stirring and drying to obtain dried basalt aggregate; S2, putting the dried basalt aggregate and the adhesive into a stirring cylinder, and uniformly stirring; S3, heating the matrix asphalt to 135-180 DEG C, adding the plant asphalt, and uniformlystirring to obtain soft asphalt; and S4, putting the soft asphalt into the stirring cylinder in the step S2, heating to 140-160 DEG C, uniformly stirring, adding the rock asphalt, continuously and uniformly stirring, adding the mineral powder, and continuously and uniformly stirring to obtain the environment-friendly asphalt mixture. The environment-friendly asphalt mixture has the advantages that the pavement performance of the mixture is not reduced, and the purposes of environmental protection and energy conservation can be achieved.
本发明公开了一种环保沥青混合料及其制备方法,涉及沥青混合料技术领域。其技术要点是:一种环保沥青混合料,包括岩沥青50‑80份;基质沥青150‑200份;植物沥青3‑5份;矿粉90‑140份;玄武岩集料500‑700份;胶黏剂5‑10份。其制备方法为:S1,将玄武岩集料投入烘干桶内,搅拌烘干,得到干燥的玄武岩集料;S2,将干燥后的玄武岩集料和胶黏剂投入搅拌缸中,搅拌均匀;S3,将基质沥青加热至135‑180℃,加入植物沥青,搅拌均匀,得到软质沥青;S4,将软质沥青投入到S2中的搅拌缸中,加热至140‑160℃,搅拌均匀,然后加入岩沥青,继续搅拌均匀,再加入矿粉并继续搅均匀,即得到环保沥青混合料。本发明环保沥青混合料具有既不降低混合料的路用性能,又能实现环保节能目的的优点。
Environment-friendly asphalt mixture and preparation method thereof
The invention discloses an environment-friendly asphalt mixture and a preparation method thereof, and relates to the technical field of asphalt mixtures. The technical key points are as follows: the environment-friendly asphalt mixture comprises 50-80 parts of rock asphalt; 150 to 200 parts of matrix asphalt; 3-5 parts of plant asphalt; 90 to 140 parts of mineral powder; 500 to 700 parts of basaltaggregate; and 5-10 parts of an adhesive. The preparation method comprises the following steps: S1, putting the basalt aggregate into a drying barrel, stirring and drying to obtain dried basalt aggregate; S2, putting the dried basalt aggregate and the adhesive into a stirring cylinder, and uniformly stirring; S3, heating the matrix asphalt to 135-180 DEG C, adding the plant asphalt, and uniformlystirring to obtain soft asphalt; and S4, putting the soft asphalt into the stirring cylinder in the step S2, heating to 140-160 DEG C, uniformly stirring, adding the rock asphalt, continuously and uniformly stirring, adding the mineral powder, and continuously and uniformly stirring to obtain the environment-friendly asphalt mixture. The environment-friendly asphalt mixture has the advantages that the pavement performance of the mixture is not reduced, and the purposes of environmental protection and energy conservation can be achieved.
本发明公开了一种环保沥青混合料及其制备方法,涉及沥青混合料技术领域。其技术要点是:一种环保沥青混合料,包括岩沥青50‑80份;基质沥青150‑200份;植物沥青3‑5份;矿粉90‑140份;玄武岩集料500‑700份;胶黏剂5‑10份。其制备方法为:S1,将玄武岩集料投入烘干桶内,搅拌烘干,得到干燥的玄武岩集料;S2,将干燥后的玄武岩集料和胶黏剂投入搅拌缸中,搅拌均匀;S3,将基质沥青加热至135‑180℃,加入植物沥青,搅拌均匀,得到软质沥青;S4,将软质沥青投入到S2中的搅拌缸中,加热至140‑160℃,搅拌均匀,然后加入岩沥青,继续搅拌均匀,再加入矿粉并继续搅均匀,即得到环保沥青混合料。本发明环保沥青混合料具有既不降低混合料的路用性能,又能实现环保节能目的的优点。
Environment-friendly asphalt mixture and preparation method thereof
一种环保沥青混合料及其制备方法
HUANG LONG (author)
2020-08-14
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Environment-friendly asphalt mixture and preparation method thereof
European Patent Office | 2021
|Environment-friendly asphalt mixture and preparation method thereof
European Patent Office | 2021
|Environment-friendly odorless asphalt mixture and preparation method thereof
European Patent Office | 2024
|Environment-friendly odorless asphalt mixture and preparation method thereof
European Patent Office | 2020
|Environment-friendly high-performance asphalt mixture and preparation method thereof
European Patent Office | 2024
|