Rammed earth wall formula and preparation method thereof
The invention provides a rammed earth wall formula. The rammed earth wall formula comprises the following components in parts by weight: 70-700 parts of raw soil; 60-600 parts of stones; 5-50 parts ofsand; 2-10 parts of lime; 2-10 parts of rubbles; 10-60 parts of water; and 1-5 parts of polypropylene fibers. According to the rammed earth wall formula, on the premise that original traditional rammed earth wall materials are reserved, the strength, durability, integrity, compactness, cracking resistance and the like of a rammed earth wall body are greatly improved, the service life of a rammedearth building is prolonged, and large economic benefits can be obtained.
本发明提供一种夯土墙配方,包括生土、石子、砂、石灰、瓦砾、水和聚丙烯纤维,各组分的重量组份为:生土70‑700份、石子60‑600份、砂5‑50份、石灰2‑10份、瓦砾2‑10份、水10‑60份以及聚丙烯纤维1‑5份。本发明的夯土墙配方在保证保留原有传统夯土墙材料的前提下,大幅度提高了夯土墙体的强度、耐久性、整体性、密实性、抗开裂性等,延长了夯土建筑的寿命,并且能够取得较大的经济效益。
Rammed earth wall formula and preparation method thereof
The invention provides a rammed earth wall formula. The rammed earth wall formula comprises the following components in parts by weight: 70-700 parts of raw soil; 60-600 parts of stones; 5-50 parts ofsand; 2-10 parts of lime; 2-10 parts of rubbles; 10-60 parts of water; and 1-5 parts of polypropylene fibers. According to the rammed earth wall formula, on the premise that original traditional rammed earth wall materials are reserved, the strength, durability, integrity, compactness, cracking resistance and the like of a rammed earth wall body are greatly improved, the service life of a rammedearth building is prolonged, and large economic benefits can be obtained.
本发明提供一种夯土墙配方,包括生土、石子、砂、石灰、瓦砾、水和聚丙烯纤维,各组分的重量组份为:生土70‑700份、石子60‑600份、砂5‑50份、石灰2‑10份、瓦砾2‑10份、水10‑60份以及聚丙烯纤维1‑5份。本发明的夯土墙配方在保证保留原有传统夯土墙材料的前提下,大幅度提高了夯土墙体的强度、耐久性、整体性、密实性、抗开裂性等,延长了夯土建筑的寿命,并且能够取得较大的经济效益。
Rammed earth wall formula and preparation method thereof
一种夯土墙配方及其制备方法
SHEN SHENG (author) / ZHANG YING (author) / WANG YAN (author) / SUN YU (author) / LIU JIAMIN (author)
2020-08-18
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2022
|Colored rammed earth wall and preparation method thereof
European Patent Office | 2023
|Reinforced structure of rammed earth wall, reinforced rammed earth wall and construction method
European Patent Office | 2023
|