The invention discloses a low-carbon ceramic tile adhesive and a tiling stability detection method, and belongs to the technical field of ceramic tile adhesives. The low-carbon ceramic tile adhesive comprises the following components by mass percentage: 5%-10% of Portland cement, 10-30% of active filler, 1%-5% of alpha semi-hydrated gypsum, 30%-50% of 40-70mesh tailing sand, 10%-30% of 80-140meshtailing sand, 0.1%-0.4% of a water-retaining agent, 0.1-4% of polymer rubber powder and 0.1-0.5% of an excitant. The invention has the advantages that: by reducing the cement consumption, carbon emission is reduced, high immersion strength is achieved, the cutting and pulling strength can be obviously improved, the stability of a tiling system is improved, the testing method is rapid, simple and consistent with an indoor application scene, the testing method provided by the invention is simple and easy to implement, hollowing caused by deformation mainly caused by temperature difference and dryness indoors is avoided, and a high coincidence degree is achieved.
本发明公开了一种低碳瓷砖胶及贴砖稳定性检测方法,属于瓷砖胶技术领域。它包括包括以下按质量百分比计的成分:硅酸盐水泥:5%~10%、活性填料:10~30%、阿尔法半水石膏:1%~5%、40‑70目尾矿砂:30%~50%、80‑140目尾矿砂:10%~30%、保水剂:0.1%~0.4%、聚合物胶粉:0.1~4%、激发剂:0.1~0.5%。本发明具有通过降低水泥用量,降低了碳排放、较高的浸水强度、可明显提高切割拉拔强度,提高贴砖体系稳定性、快速、简单、吻合室内应用场景的测试方法,本发明提出的测试方法简单易行,针对室内主要由温差及干燥引起形变导致空鼓掉,有较高的吻合度。
Low-carbon ceramic tile adhesive and tiling stability detection method
The invention discloses a low-carbon ceramic tile adhesive and a tiling stability detection method, and belongs to the technical field of ceramic tile adhesives. The low-carbon ceramic tile adhesive comprises the following components by mass percentage: 5%-10% of Portland cement, 10-30% of active filler, 1%-5% of alpha semi-hydrated gypsum, 30%-50% of 40-70mesh tailing sand, 10%-30% of 80-140meshtailing sand, 0.1%-0.4% of a water-retaining agent, 0.1-4% of polymer rubber powder and 0.1-0.5% of an excitant. The invention has the advantages that: by reducing the cement consumption, carbon emission is reduced, high immersion strength is achieved, the cutting and pulling strength can be obviously improved, the stability of a tiling system is improved, the testing method is rapid, simple and consistent with an indoor application scene, the testing method provided by the invention is simple and easy to implement, hollowing caused by deformation mainly caused by temperature difference and dryness indoors is avoided, and a high coincidence degree is achieved.
本发明公开了一种低碳瓷砖胶及贴砖稳定性检测方法,属于瓷砖胶技术领域。它包括包括以下按质量百分比计的成分:硅酸盐水泥:5%~10%、活性填料:10~30%、阿尔法半水石膏:1%~5%、40‑70目尾矿砂:30%~50%、80‑140目尾矿砂:10%~30%、保水剂:0.1%~0.4%、聚合物胶粉:0.1~4%、激发剂:0.1~0.5%。本发明具有通过降低水泥用量,降低了碳排放、较高的浸水强度、可明显提高切割拉拔强度,提高贴砖体系稳定性、快速、简单、吻合室内应用场景的测试方法,本发明提出的测试方法简单易行,针对室内主要由温差及干燥引起形变导致空鼓掉,有较高的吻合度。
Low-carbon ceramic tile adhesive and tiling stability detection method
一种低碳瓷砖胶及贴砖稳定性检测方法