A platform for research: civil engineering, architecture and urbanism
Gypsum-based wall leveling material as well as preparation method and use method thereof
The invention relates to a gypsum-based wall leveling material as well as a preparation method and a use method thereof. The wall leveling material is prepared from the following raw materials in parts by mass: 55-70 parts of semi-hydrated gypsum; 8-20 parts of fly ash; 4-8 parts of an admixture; 4-8 parts of calcium hydroxide; 3-6 parts of zeolite; 0.2-0.5 part of a water retaining agent; and 0.05-0.1 part of a retarder; wherein the admixture is selected from one or two of silica fume or metakaolin. The gypsum-based wall leveling material provided by the invention does not need cement, redispersible rubber powder and a water repellent, can also have good water resistance, can maintain good mechanical properties in a high-humidity environment, can also solve the problems of hollowing and cracking of a wall surface, and is low in cost and easier to apply and popularize.
本发明涉及一种石膏基墙体找平材料及其制备方法和使用方法。以质量份计,其制备原料包括:半水石膏55份‑70份;粉煤灰8份‑20份;掺合料4份‑8份;氢氧化钙4份‑8份;沸石3份‑6份;保水剂0.2份‑0.5份;缓凝剂0.05份‑0.1份;所述掺合料选自硅灰或偏高岭土中的一种或两种。本发明所述的石膏基墙体找平材料非必须使用水泥、可再分散性胶粉和憎水剂,也可以具有较好的耐水性能,在高湿度环境下,可以保持良好的力学性能,同时,可以解决墙面空鼓、开裂难题,并且成本低,更易应用推广。
Gypsum-based wall leveling material as well as preparation method and use method thereof
The invention relates to a gypsum-based wall leveling material as well as a preparation method and a use method thereof. The wall leveling material is prepared from the following raw materials in parts by mass: 55-70 parts of semi-hydrated gypsum; 8-20 parts of fly ash; 4-8 parts of an admixture; 4-8 parts of calcium hydroxide; 3-6 parts of zeolite; 0.2-0.5 part of a water retaining agent; and 0.05-0.1 part of a retarder; wherein the admixture is selected from one or two of silica fume or metakaolin. The gypsum-based wall leveling material provided by the invention does not need cement, redispersible rubber powder and a water repellent, can also have good water resistance, can maintain good mechanical properties in a high-humidity environment, can also solve the problems of hollowing and cracking of a wall surface, and is low in cost and easier to apply and popularize.
本发明涉及一种石膏基墙体找平材料及其制备方法和使用方法。以质量份计,其制备原料包括:半水石膏55份‑70份;粉煤灰8份‑20份;掺合料4份‑8份;氢氧化钙4份‑8份;沸石3份‑6份;保水剂0.2份‑0.5份;缓凝剂0.05份‑0.1份;所述掺合料选自硅灰或偏高岭土中的一种或两种。本发明所述的石膏基墙体找平材料非必须使用水泥、可再分散性胶粉和憎水剂,也可以具有较好的耐水性能,在高湿度环境下,可以保持良好的力学性能,同时,可以解决墙面空鼓、开裂难题,并且成本低,更易应用推广。
Gypsum-based wall leveling material as well as preparation method and use method thereof
石膏基墙体找平材料及其制备方法和使用方法
LI YANMEI (author) / TANG ZHENZHONG (author) / PENG LUXI (author) / LIU KAI (author)
2020-11-17
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Gypsum-based self-leveling material and preparation method thereof
European Patent Office | 2024
|Gypsum self-leveling material and preparation method thereof
European Patent Office | 2020
|Composite gypsum self-leveling ground system leveling material and preparation method thereof
European Patent Office | 2023
|Gypsum-based self-leveling floor material and preparation method thereof
European Patent Office | 2020
|Anhydrous gypsum self-leveling material and preparation method thereof
European Patent Office | 2022
|