Purification method of boron carbide micro-powder, boron carbide ceramic and preparation method of boron carbide ceramic
The invention discloses a boron carbide micro-powder purification method, a boron carbide ceramic and a preparation method of the boron carbide ceramic. The boron carbide micro-powder purification method comprises the following steps: carrying out homogenizing grinding, vacuum heat treatment purification and secondary grinding on the basis of commercially available W3.5 series boron carbide micro-powder raw material, and carrying out drying and powdering on boron carbide slurry in a spray granulation mode. The boron carbide ceramic is composed of the following components: boron carbide micro-powder, liquid carbon black, submicron aluminum nitride micro-powder, a titanate coupling agent, water-soluble phenolic resin, water-soluble acrylic acid glue, polyethylene glycol, glycerol, deionizedwater, whisker type multi-walled carbon nanotubes and Ti--Si-C ternary MAX phase micro-powder. The preparation method of the boron carbide ceramic comprises the following steps: weighing the components, carrying out high-speed ball-milling pulping, carrying out spray granulation, pressing a green body, and carrying out pressureless sintering. The problem that in the prior art, the purity of boroncarbide micro-powder is not high is solved, and meanwhile pressureless sintering preparation of the boron carbide ceramic is achieved.
本发明公开了碳化硼微粉提纯方法、碳化硼陶瓷及碳化硼陶瓷的制备方法。碳化硼微粉提纯方法,以市售W3.5系列的碳化硼微粉原料为基础进行均化研磨、真空热处理提纯、二次研磨,将碳化硼浆料采用喷雾造粒的方式进行烘干制粉。碳化硼陶瓷由以下成分构成,碳化硼微粉、液体炭黑、亚微米氮化铝微粉、钛酸酯偶联剂、水溶性酚醛树脂、水溶性丙烯酸胶、聚乙二醇、甘油、去离子水、晶须型多壁碳纳米管、Ti‑‑Si‑C三元MAX相微粉。碳化硼陶瓷制备方法,按组分称重后进行高速球磨制浆、喷雾造粒、生坯压制、无压烧成。解决了现有技术中碳化硼微粉纯度不高的问题,同时实现了碳化硼陶瓷的无压烧结制备。
Purification method of boron carbide micro-powder, boron carbide ceramic and preparation method of boron carbide ceramic
The invention discloses a boron carbide micro-powder purification method, a boron carbide ceramic and a preparation method of the boron carbide ceramic. The boron carbide micro-powder purification method comprises the following steps: carrying out homogenizing grinding, vacuum heat treatment purification and secondary grinding on the basis of commercially available W3.5 series boron carbide micro-powder raw material, and carrying out drying and powdering on boron carbide slurry in a spray granulation mode. The boron carbide ceramic is composed of the following components: boron carbide micro-powder, liquid carbon black, submicron aluminum nitride micro-powder, a titanate coupling agent, water-soluble phenolic resin, water-soluble acrylic acid glue, polyethylene glycol, glycerol, deionizedwater, whisker type multi-walled carbon nanotubes and Ti--Si-C ternary MAX phase micro-powder. The preparation method of the boron carbide ceramic comprises the following steps: weighing the components, carrying out high-speed ball-milling pulping, carrying out spray granulation, pressing a green body, and carrying out pressureless sintering. The problem that in the prior art, the purity of boroncarbide micro-powder is not high is solved, and meanwhile pressureless sintering preparation of the boron carbide ceramic is achieved.
本发明公开了碳化硼微粉提纯方法、碳化硼陶瓷及碳化硼陶瓷的制备方法。碳化硼微粉提纯方法,以市售W3.5系列的碳化硼微粉原料为基础进行均化研磨、真空热处理提纯、二次研磨,将碳化硼浆料采用喷雾造粒的方式进行烘干制粉。碳化硼陶瓷由以下成分构成,碳化硼微粉、液体炭黑、亚微米氮化铝微粉、钛酸酯偶联剂、水溶性酚醛树脂、水溶性丙烯酸胶、聚乙二醇、甘油、去离子水、晶须型多壁碳纳米管、Ti‑‑Si‑C三元MAX相微粉。碳化硼陶瓷制备方法,按组分称重后进行高速球磨制浆、喷雾造粒、生坯压制、无压烧成。解决了现有技术中碳化硼微粉纯度不高的问题,同时实现了碳化硼陶瓷的无压烧结制备。
Purification method of boron carbide micro-powder, boron carbide ceramic and preparation method of boron carbide ceramic
碳化硼微粉提纯方法、碳化硼陶瓷及碳化硼陶瓷制备方法
SHI YANMIN (author) / XU ZHENGPING (author) / LONG CHENGYONG (author) / CAO JIANWU (author) / XU NAI'AN (author)
2020-12-25
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2024
|