Ceramic raw material formula for manufacturing tableware and preparation method thereof
The invention provides a ceramic raw material formula for manufacturing tableware and a preparation method thereof. The ceramic raw material formula comprises the following raw materials in parts by weight: 22-28 parts of aluminum oxide, 15-18 parts of silicon nitride, 6-9 parts of talcum powder, 14-17 parts of dolomite, 15-18 parts of magnesium oxide, 12-15 parts of bentonite, 7-10 parts of sepiolite, 10-14 parts of calcite, 7-10 parts of zeolite, 17-20 parts of volcanic rock, 12-16 parts of coal ash and 13-18 parts of water. According to the ceramic raw material formula for manufacturing thetableware and the preparation method of the ceramic raw material formula, the overall adhesion degree of the ceramic tableware is improved, the hardness is not lost, the overall toughness of the ceramic is improved, and the ceramic tableware is not prone to breakage; and the wear resistance of the ceramic tableware is high; the strength of the ceramic tableware is enhanced, and the weight of theceramic tableware is not increased; the wear resistance and the corrosion resistance of the ceramic tableware are improved, and the tableware cannot be worn or corroded to change color even if the tableware is used for a long time; and the weight of the ceramic tableware is reduced, and the light weight is ensured.
本发明提供了一种用于制作餐具的陶瓷原料配方及其制备方法,其原料及配比如下:氧化铝22‑28份、氮化硅15‑18份、滑石粉6‑9份、白云土14‑17份、氧化镁15‑18份、膨润土12‑15份、海泡石7‑10份、方解石10‑14份、沸石7‑10份、火山岩17‑20份、煤灰12‑16份、水13‑18份。本专利所述的一种用于制作餐具的陶瓷原料配方及其制备方法,提高了陶瓷餐具的整体粘合度,且不丧失硬度,增加了陶瓷的整体韧性,使其不易破碎;使得陶瓷餐具耐磨性强;增强了陶瓷餐具强度,且不会增加陶瓷餐具的重量;提高了陶瓷餐具的耐磨损和抗腐蚀性能,可保证即使餐具长期使用,也不会磨损或被腐蚀变色;减轻了陶瓷餐具的重量,保证其质地轻盈。
Ceramic raw material formula for manufacturing tableware and preparation method thereof
The invention provides a ceramic raw material formula for manufacturing tableware and a preparation method thereof. The ceramic raw material formula comprises the following raw materials in parts by weight: 22-28 parts of aluminum oxide, 15-18 parts of silicon nitride, 6-9 parts of talcum powder, 14-17 parts of dolomite, 15-18 parts of magnesium oxide, 12-15 parts of bentonite, 7-10 parts of sepiolite, 10-14 parts of calcite, 7-10 parts of zeolite, 17-20 parts of volcanic rock, 12-16 parts of coal ash and 13-18 parts of water. According to the ceramic raw material formula for manufacturing thetableware and the preparation method of the ceramic raw material formula, the overall adhesion degree of the ceramic tableware is improved, the hardness is not lost, the overall toughness of the ceramic is improved, and the ceramic tableware is not prone to breakage; and the wear resistance of the ceramic tableware is high; the strength of the ceramic tableware is enhanced, and the weight of theceramic tableware is not increased; the wear resistance and the corrosion resistance of the ceramic tableware are improved, and the tableware cannot be worn or corroded to change color even if the tableware is used for a long time; and the weight of the ceramic tableware is reduced, and the light weight is ensured.
本发明提供了一种用于制作餐具的陶瓷原料配方及其制备方法,其原料及配比如下:氧化铝22‑28份、氮化硅15‑18份、滑石粉6‑9份、白云土14‑17份、氧化镁15‑18份、膨润土12‑15份、海泡石7‑10份、方解石10‑14份、沸石7‑10份、火山岩17‑20份、煤灰12‑16份、水13‑18份。本专利所述的一种用于制作餐具的陶瓷原料配方及其制备方法,提高了陶瓷餐具的整体粘合度,且不丧失硬度,增加了陶瓷的整体韧性,使其不易破碎;使得陶瓷餐具耐磨性强;增强了陶瓷餐具强度,且不会增加陶瓷餐具的重量;提高了陶瓷餐具的耐磨损和抗腐蚀性能,可保证即使餐具长期使用,也不会磨损或被腐蚀变色;减轻了陶瓷餐具的重量,保证其质地轻盈。
Ceramic raw material formula for manufacturing tableware and preparation method thereof
一种用于制作餐具的陶瓷原料配方及其制备方法
LIU SHAOPENG (author)
2021-01-08
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Antibacterial ceramic material, preparation method and application thereof, and tableware
European Patent Office | 2023
|European Patent Office | 2021
|Manufacturing method of induction heating ceramic tableware
European Patent Office | 2015
|