Mining high-water high-strength filling material and preparation method thereof
The invention discloses a mining high-water high-strength filling material and a preparation method thereof. The mining high-water high-strength filling material is prepared from, by mass, a componentA and a component B. The component A includes, by mass, 50-70 parts of sulphoaluminate cement, 5-10 parts of fly ash, 1-10 parts of sodium bentonite, 1-5 parts of retarder and 1-5 parts of suspendingagent; and the component B includes: 5-10 parts of gypsum powder, 2-5 parts of quick lime, 1-5 parts of kaolin, 5-30 parts of quartz powder and 1-10 parts of a composite additive; and the raw materials of the component A and the component B are mixed in proportion and uniformly stirred to obtain the mining high-water-content high-strength filling material. The prepared material has the advantagesthat the setting time can be adjusted from ten minutes to several hours, and the compressive strength is high.
本发明公开了一种矿用高水高强度充填材料及制备方法,矿用高水高强度充填材料的制备原料包括A组分和B组分,以质量份数计,A组分包括:硫铝酸盐水泥50‑70份,粉煤灰5‑10份,钠基膨润土1‑10份,缓凝剂1‑5份,悬浮剂1‑5份;B组分包括:石膏粉5‑10份,生石灰2‑5份,高岭土1‑5份,石英粉5‑30份,复合添加剂1‑10份,将A组分和B组分的原料按比例混合,搅拌均匀,即得到矿用高水高强度充填材料。本发明所制备材料具有凝结时间可由十分钟至数小时调节,抗压强度高的优势。
Mining high-water high-strength filling material and preparation method thereof
The invention discloses a mining high-water high-strength filling material and a preparation method thereof. The mining high-water high-strength filling material is prepared from, by mass, a componentA and a component B. The component A includes, by mass, 50-70 parts of sulphoaluminate cement, 5-10 parts of fly ash, 1-10 parts of sodium bentonite, 1-5 parts of retarder and 1-5 parts of suspendingagent; and the component B includes: 5-10 parts of gypsum powder, 2-5 parts of quick lime, 1-5 parts of kaolin, 5-30 parts of quartz powder and 1-10 parts of a composite additive; and the raw materials of the component A and the component B are mixed in proportion and uniformly stirred to obtain the mining high-water-content high-strength filling material. The prepared material has the advantagesthat the setting time can be adjusted from ten minutes to several hours, and the compressive strength is high.
本发明公开了一种矿用高水高强度充填材料及制备方法,矿用高水高强度充填材料的制备原料包括A组分和B组分,以质量份数计,A组分包括:硫铝酸盐水泥50‑70份,粉煤灰5‑10份,钠基膨润土1‑10份,缓凝剂1‑5份,悬浮剂1‑5份;B组分包括:石膏粉5‑10份,生石灰2‑5份,高岭土1‑5份,石英粉5‑30份,复合添加剂1‑10份,将A组分和B组分的原料按比例混合,搅拌均匀,即得到矿用高水高强度充填材料。本发明所制备材料具有凝结时间可由十分钟至数小时调节,抗压强度高的优势。
Mining high-water high-strength filling material and preparation method thereof
一种矿用高水高强度充填材料及制备方法
ZHAO TENGFEI (author) / GENG YAOQIANG (author) / LIANG QIAN (author) / LI XIANLIANG (author) / AN XIUYU (author) / ZHANG YUANZHEN (author)
2021-01-22
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Mining gob-side entry retaining high-water filling material and preparation method thereof
European Patent Office | 2020
|European Patent Office | 2024
|High-strength mineral inorganic foaming filling material and preparation method thereof
European Patent Office | 2021
|European Patent Office | 2024
|High-strength mineral-based inorganic injection filling material and preparation method thereof
European Patent Office | 2022
|