Porcelain matte archaized brick and manufacturing method thereof
The invention discloses a porcelain matte archaized brick and a manufacturing method thereof, and the manufacturing method of the porcelain matte archaized brick comprises the following steps: pressing, molding and drying green body powder to obtain an archaized brick biscuit; applying low-gloss opacified ground coat to the archaized brick biscuit to obtain a ground coat layer; printing a decorative pattern on the ground coat layer in an ink-jet mode to obtain a decorative pattern layer; applying matte transparent archaistic surface glaze to the decorative pattern layer to obtain an archaisticsurface glaze layer; and performing archaistic processing, and placing the mixture in a roller kiln for firing. By applying the low-gloss opacified ground coat to the archaized brick biscuit, the high-temperature loading capacity can be guaranteed, the brick shape can be improved, the flatness of the brick surface can be improved, and the influence on the performances such as the brick shape, thestick grain and the corner falling can be reduced; and then, pattern decoration is carried out on the low-gloss opacified ground coat, and finally, the decorative pattern layer is covered with the matte antique finish coat, so that the design and color of the decorative pattern are effectively protected, the texture is effectively adjusted, and the wear resistance of the antique brick is improved.
本发明公开了一种瓷质哑光仿古砖及其制造方法,瓷质哑光仿古砖的制造方法,包括:将坯体粉料压制成型并干燥,获得仿古砖素坯;在仿古砖素坯上施加低光泽乳浊底釉,获得底釉层;在底釉层上喷墨打印装饰图案,获得装饰图案层;在装饰图案层上施加哑光透明仿古面釉,获得仿古面釉层;进行仿古加工,并置入辊道窑烧成。通过在仿古砖素坯上先施加低光泽乳浊底釉,进而可以先保障高温载荷能力、改善砖形、提高砖面的平整度,且降低对砖形、棍棒纹、掉角等性能的影响;然后,在低光泽乳浊底釉上进行图案装饰,最后再在所述装饰图案层上覆盖哑光仿古面釉,进而有效的保护了装饰图案花色,并有效调整质感和提升仿古砖的耐磨性。
Porcelain matte archaized brick and manufacturing method thereof
The invention discloses a porcelain matte archaized brick and a manufacturing method thereof, and the manufacturing method of the porcelain matte archaized brick comprises the following steps: pressing, molding and drying green body powder to obtain an archaized brick biscuit; applying low-gloss opacified ground coat to the archaized brick biscuit to obtain a ground coat layer; printing a decorative pattern on the ground coat layer in an ink-jet mode to obtain a decorative pattern layer; applying matte transparent archaistic surface glaze to the decorative pattern layer to obtain an archaisticsurface glaze layer; and performing archaistic processing, and placing the mixture in a roller kiln for firing. By applying the low-gloss opacified ground coat to the archaized brick biscuit, the high-temperature loading capacity can be guaranteed, the brick shape can be improved, the flatness of the brick surface can be improved, and the influence on the performances such as the brick shape, thestick grain and the corner falling can be reduced; and then, pattern decoration is carried out on the low-gloss opacified ground coat, and finally, the decorative pattern layer is covered with the matte antique finish coat, so that the design and color of the decorative pattern are effectively protected, the texture is effectively adjusted, and the wear resistance of the antique brick is improved.
本发明公开了一种瓷质哑光仿古砖及其制造方法,瓷质哑光仿古砖的制造方法,包括:将坯体粉料压制成型并干燥,获得仿古砖素坯;在仿古砖素坯上施加低光泽乳浊底釉,获得底釉层;在底釉层上喷墨打印装饰图案,获得装饰图案层;在装饰图案层上施加哑光透明仿古面釉,获得仿古面釉层;进行仿古加工,并置入辊道窑烧成。通过在仿古砖素坯上先施加低光泽乳浊底釉,进而可以先保障高温载荷能力、改善砖形、提高砖面的平整度,且降低对砖形、棍棒纹、掉角等性能的影响;然后,在低光泽乳浊底釉上进行图案装饰,最后再在所述装饰图案层上覆盖哑光仿古面釉,进而有效的保护了装饰图案花色,并有效调整质感和提升仿古砖的耐磨性。
Porcelain matte archaized brick and manufacturing method thereof
一种瓷质哑光仿古砖及其制造方法
DENG XINGZHI (author) / SHEN RONGWEI (author) / ZENG SHAOXIONG (author) / XU CHAO (author) / WANG ZHIJUN (author)
2021-02-23
Patent
Electronic Resource
Chinese
European Patent Office | 2020
|Preparation method of matte pea green glaze archaized porcelain
European Patent Office | 2020
|European Patent Office | 2024
|Porcelain archaized brick with silk surface and preparation method thereof
European Patent Office | 2020
|Archaized brick framework and archaized brick pressing production method
European Patent Office | 2021
|