The invention provides corrosion-resistant concrete for an offshore sewage pipeline and a preparation method of the corrosion-resistant concrete. The concrete comprises the following components: 150-200 parts of ordinary Portland cement, 180-220 parts of mineral powder, 50-70 parts of fly ash, 15-30 parts of silica fume, 12-20 parts of desulfurized gypsum, 5-9 parts of a polycarboxylic acid high-performance water reducing agent, 12-20 parts of an expanding agent, 2-6 parts of basalt fibers, 0.05-0.8 part of modified multi-walled carbon nanotubes, 600-800 parts of sand, 950-1100 parts of stonesand 160-175 parts of water. The prepared corrosion-resistant concrete for the offshore sewage pipeline has good mechanical properties and corrosion resistance, the quality of the offshore sewage pipeline is improved, and the service life of the offshore sewage pipeline is prolonged.
本发明提供一种近海污水管道用耐腐蚀混凝土及其制备方法,其按重量份计,包含有以下组分:普通硅酸盐水泥150‑200份、矿粉180‑220份、粉煤灰50‑70份、硅灰15‑30份、脱硫石膏12‑20份、聚羧酸高性能减水剂5‑9份、膨胀剂12‑20份、玄武岩纤维2‑6份、改性多壁碳纳米管0.05‑0.8份、砂子600‑800份、石子950‑1100份和水160‑175份;本发明制备获得的近海污水管道用耐腐蚀混凝土具有良好的力学性能和防腐性能,提高近海污水管道的质量和使用寿命。
Corrosion-resistant concrete for offshore sewage pipeline and preparation method of corrosion-resistant concrete
The invention provides corrosion-resistant concrete for an offshore sewage pipeline and a preparation method of the corrosion-resistant concrete. The concrete comprises the following components: 150-200 parts of ordinary Portland cement, 180-220 parts of mineral powder, 50-70 parts of fly ash, 15-30 parts of silica fume, 12-20 parts of desulfurized gypsum, 5-9 parts of a polycarboxylic acid high-performance water reducing agent, 12-20 parts of an expanding agent, 2-6 parts of basalt fibers, 0.05-0.8 part of modified multi-walled carbon nanotubes, 600-800 parts of sand, 950-1100 parts of stonesand 160-175 parts of water. The prepared corrosion-resistant concrete for the offshore sewage pipeline has good mechanical properties and corrosion resistance, the quality of the offshore sewage pipeline is improved, and the service life of the offshore sewage pipeline is prolonged.
本发明提供一种近海污水管道用耐腐蚀混凝土及其制备方法,其按重量份计,包含有以下组分:普通硅酸盐水泥150‑200份、矿粉180‑220份、粉煤灰50‑70份、硅灰15‑30份、脱硫石膏12‑20份、聚羧酸高性能减水剂5‑9份、膨胀剂12‑20份、玄武岩纤维2‑6份、改性多壁碳纳米管0.05‑0.8份、砂子600‑800份、石子950‑1100份和水160‑175份;本发明制备获得的近海污水管道用耐腐蚀混凝土具有良好的力学性能和防腐性能,提高近海污水管道的质量和使用寿命。
Corrosion-resistant concrete for offshore sewage pipeline and preparation method of corrosion-resistant concrete
一种近海污水管道用耐腐蚀混凝土及其制备方法
WANG JUNFENG (author)
2021-04-02
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2024
|