Kitchen and toilet brick-smashing-free quick repair system and method thereof
The invention provides a kitchen and toilet brick-smashing-free quick repair system and a method thereof. The construction method of the kitchen and toilet brick-smashing-free quick repair system comprises the following steps that grouting is conducted on a leakage point, it needs to be determined that no water pipe or line pipe exists below a ceramic tile at the corresponding position near the leakage point, a phi 14 glass tapper is used for tapping the ceramic tile, the ceramic tile is taken out for standby application (sticking back during joint filling), then a hole is drilled to a bottom plate through a phi 14 percussion drill, an A10 water stop needle head is installed, acrylate or a capillary crystalline brick-smashing-free waterproof agent is poured through a double-liquid grouting machine, and leakage point blocking is conducted. According to the construction method, on the premise that the upper and lower water pipes of the toilet are not damaged, a whole-system solving method is creatively provided, the aim of treating both symptoms and root causes is achieved in a multi-pipe mode, the problem of water leakage can be rapidly and thoroughly solved in a low-cost mode without smashing bricks, generation of construction waste is avoided, normal life of residents is not affected, and meanwhile, the building structure is prevented from being damaged.
本发明提供了一种厨卫间免砸砖快修系统及其方法,该厨卫间免砸砖快修系统施工方法包括如下步骤:漏点注浆,在漏点附近对应部位需确定瓷砖下面无水管、线管,用φ14玻璃开孔器在瓷砖上开孔,取出备用(填缝时粘回),再用φ14冲击钻钻孔至底板,安装A10止水针头,用双液注浆机灌注丙烯酸盐或渗透结晶免砸砖防水剂,进行漏点封堵。本发明在卫生间上下水管无破损的前提下,创造性地提出全系统地解决方法,通过多管齐下的方式,来达到标本兼治目的,可以快速、免砸砖、低成本地彻底解决渗漏水难题,避免建筑垃圾的产生,不影响居民的正常生活,同时也避免建筑结构受到损坏。
Kitchen and toilet brick-smashing-free quick repair system and method thereof
The invention provides a kitchen and toilet brick-smashing-free quick repair system and a method thereof. The construction method of the kitchen and toilet brick-smashing-free quick repair system comprises the following steps that grouting is conducted on a leakage point, it needs to be determined that no water pipe or line pipe exists below a ceramic tile at the corresponding position near the leakage point, a phi 14 glass tapper is used for tapping the ceramic tile, the ceramic tile is taken out for standby application (sticking back during joint filling), then a hole is drilled to a bottom plate through a phi 14 percussion drill, an A10 water stop needle head is installed, acrylate or a capillary crystalline brick-smashing-free waterproof agent is poured through a double-liquid grouting machine, and leakage point blocking is conducted. According to the construction method, on the premise that the upper and lower water pipes of the toilet are not damaged, a whole-system solving method is creatively provided, the aim of treating both symptoms and root causes is achieved in a multi-pipe mode, the problem of water leakage can be rapidly and thoroughly solved in a low-cost mode without smashing bricks, generation of construction waste is avoided, normal life of residents is not affected, and meanwhile, the building structure is prevented from being damaged.
本发明提供了一种厨卫间免砸砖快修系统及其方法,该厨卫间免砸砖快修系统施工方法包括如下步骤:漏点注浆,在漏点附近对应部位需确定瓷砖下面无水管、线管,用φ14玻璃开孔器在瓷砖上开孔,取出备用(填缝时粘回),再用φ14冲击钻钻孔至底板,安装A10止水针头,用双液注浆机灌注丙烯酸盐或渗透结晶免砸砖防水剂,进行漏点封堵。本发明在卫生间上下水管无破损的前提下,创造性地提出全系统地解决方法,通过多管齐下的方式,来达到标本兼治目的,可以快速、免砸砖、低成本地彻底解决渗漏水难题,避免建筑垃圾的产生,不影响居民的正常生活,同时也避免建筑结构受到损坏。
Kitchen and toilet brick-smashing-free quick repair system and method thereof
一种厨卫间免砸砖快修系统及其方法
XIA XINHUA (author) / FU ZUJIN (author)
2021-05-04
Patent
Electronic Resource
Chinese
IPC:
E04B
Allgemeine Baukonstruktionen
,
GENERAL BUILDING CONSTRUCTIONS
Moisture-curing liquid waterproof repair liquid for brick-smashing-free leaking stoppage
European Patent Office | 2020
|