Underground engineering construction sludge environment-friendly baking-free brick and production method thereof
The invention relates to the field of buildings, in particular to an underground engineering construction sludge environment-friendly baking-free brick and a production method thereof. The environment-friendly baking-free brick is prepared from the following raw materials in parts by weight: 60%-70% of underground engineering construction sludge, 8%-10% of underground engineering construction solid residues, 10%-15% of CaO, 6%-8% of 425 ordinary Portland cement, 0.1%-0.5% of A type biological enzyme and 5%-10% of H2O. According to the environment-friendly baking-free brick for the underground engineering construction sludge, the problem that the environment is seriously affected due to the fact that traditional underground engineering construction sludge treatment needs transportation, stacking, landfill and other methods is solved, the underground engineering construction sludge is well utilized in a recycling, harmless and reducing mode, waste is treated and utilized, and the self value is exerted, resources are saved, and multiple purposes are achieved.
本发明涉及建筑领域,具体涉及的是一种地下工程施工污泥环保免烧砖及其生产方法,由如下重量份的原料制得:由如下重量份的原料制得:地下工程施工污泥60%‑70%、地下工程施工固体渣料8%‑10%、Cao10%‑15%、425普通硅酸盐水泥6%‑8%、A型生物酶0.1%‑0.5%、H2O5%‑10%,本发明的地下工程施工污泥环保免烧砖解决了传统地下工程施工污泥处理需要运输、堆放、填埋等方法而严重影响环境的难题,使地下工程施工污泥得到了很好的资源化、无害化以及减量化的利用,不仅使废物得到处理和利用,发挥了自身的价值,也节省了资源,一举多得。
Underground engineering construction sludge environment-friendly baking-free brick and production method thereof
The invention relates to the field of buildings, in particular to an underground engineering construction sludge environment-friendly baking-free brick and a production method thereof. The environment-friendly baking-free brick is prepared from the following raw materials in parts by weight: 60%-70% of underground engineering construction sludge, 8%-10% of underground engineering construction solid residues, 10%-15% of CaO, 6%-8% of 425 ordinary Portland cement, 0.1%-0.5% of A type biological enzyme and 5%-10% of H2O. According to the environment-friendly baking-free brick for the underground engineering construction sludge, the problem that the environment is seriously affected due to the fact that traditional underground engineering construction sludge treatment needs transportation, stacking, landfill and other methods is solved, the underground engineering construction sludge is well utilized in a recycling, harmless and reducing mode, waste is treated and utilized, and the self value is exerted, resources are saved, and multiple purposes are achieved.
本发明涉及建筑领域,具体涉及的是一种地下工程施工污泥环保免烧砖及其生产方法,由如下重量份的原料制得:由如下重量份的原料制得:地下工程施工污泥60%‑70%、地下工程施工固体渣料8%‑10%、Cao10%‑15%、425普通硅酸盐水泥6%‑8%、A型生物酶0.1%‑0.5%、H2O5%‑10%,本发明的地下工程施工污泥环保免烧砖解决了传统地下工程施工污泥处理需要运输、堆放、填埋等方法而严重影响环境的难题,使地下工程施工污泥得到了很好的资源化、无害化以及减量化的利用,不仅使废物得到处理和利用,发挥了自身的价值,也节省了资源,一举多得。
Underground engineering construction sludge environment-friendly baking-free brick and production method thereof
一种地下工程施工污泥环保免烧砖及其生产方法
DENG WEICHENG (author)
2021-07-16
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2021
|Environment-friendly baking-free brick and preparation process thereof
European Patent Office | 2023
|Environment-friendly regenerated baking-free brick and preparation method thereof
European Patent Office | 2020
|European Patent Office | 2020
|