Method for producing calcium fluoride product by using calcium fluoride sludge
The invention provides a method for producing a calcium fluoride product by using calcium fluoride sludge. The calcium fluoride product is prepared from the following raw materials: 5-15 parts by weight of feldspar, 6-17 parts by weight of kaolin, 5-14 parts by weight of calcium fluoride sludge, 3-9 parts by weight of quartz, 4-10 parts by weight of pottery stone particles, 2-7 parts by weight of a tackifier, 2-6 parts by weight of starch, 2-6 parts by weight of baking soda and 2-5 parts by weight of glue. The feldspar, the kaolin, the quartz and the pottery stone particles are arranged, the feldspar, the kaolin, the quartz and the pottery stone particles are smashed and stirred with the calcium fluoride sludge, after stirring is completed, a raw material for preparing the calcium fluoride product can be formed, the activity of the calcium fluoride product can be improved, and the quality of the calcium fluoride product can be improved; and the overall viscosity of the raw materials can be improved through the added tackifier; and the quality of the calcium fluoride product is further improved, and the service life of the finished product is prolonged.
本发明提供了一种利用氟化钙污泥生产氟化钙制品的方法,其由以下原料制成:长石5‑15重量份、高岭土6‑17重量份、氟化钙污泥5‑14重量份、石英3‑9重量份、陶石粒4‑10重量份、增粘剂2‑7重量份、淀粉2‑6重量份、小苏打2‑6重量份、胶水2‑5重量份。本发明通过设置的长石、高岭土、石英、陶石粒,将长石、高岭土、石英、陶石粒粉碎,并与氟化钙污泥搅拌,搅拌完成之后能够形成制作氟化钙制品的原料,能够提高氟化钙制品的活性,提高质量,通过添加的增粘剂,能够提高原料的整体粘度,进一步提升氟化钙制品质量,提高成品的使用寿命。
Method for producing calcium fluoride product by using calcium fluoride sludge
The invention provides a method for producing a calcium fluoride product by using calcium fluoride sludge. The calcium fluoride product is prepared from the following raw materials: 5-15 parts by weight of feldspar, 6-17 parts by weight of kaolin, 5-14 parts by weight of calcium fluoride sludge, 3-9 parts by weight of quartz, 4-10 parts by weight of pottery stone particles, 2-7 parts by weight of a tackifier, 2-6 parts by weight of starch, 2-6 parts by weight of baking soda and 2-5 parts by weight of glue. The feldspar, the kaolin, the quartz and the pottery stone particles are arranged, the feldspar, the kaolin, the quartz and the pottery stone particles are smashed and stirred with the calcium fluoride sludge, after stirring is completed, a raw material for preparing the calcium fluoride product can be formed, the activity of the calcium fluoride product can be improved, and the quality of the calcium fluoride product can be improved; and the overall viscosity of the raw materials can be improved through the added tackifier; and the quality of the calcium fluoride product is further improved, and the service life of the finished product is prolonged.
本发明提供了一种利用氟化钙污泥生产氟化钙制品的方法,其由以下原料制成:长石5‑15重量份、高岭土6‑17重量份、氟化钙污泥5‑14重量份、石英3‑9重量份、陶石粒4‑10重量份、增粘剂2‑7重量份、淀粉2‑6重量份、小苏打2‑6重量份、胶水2‑5重量份。本发明通过设置的长石、高岭土、石英、陶石粒,将长石、高岭土、石英、陶石粒粉碎,并与氟化钙污泥搅拌,搅拌完成之后能够形成制作氟化钙制品的原料,能够提高氟化钙制品的活性,提高质量,通过添加的增粘剂,能够提高原料的整体粘度,进一步提升氟化钙制品质量,提高成品的使用寿命。
Method for producing calcium fluoride product by using calcium fluoride sludge
一种利用氟化钙污泥生产氟化钙制品的方法
LI YAN (author) / XIE GUOQING (author) / XIE BAOYU (author) / NIE HUI (author)
2021-08-06
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
METHOD OF PRODUCING MINERALIZER BASED ON CALCIUM FLUORIDE
European Patent Office | 2020
|Cement-based dry hard concrete using calcium fluoride sludge as aggregate
European Patent Office | 2021
|Application of Reutilization Technology to Calcium Fluoride Sludge from Semiconductor Manufacturers
Taylor & Francis Verlag | 2011
|