Formula of autoclaved aerated concrete block
The formula of an autoclaved aerated concrete block comprises aluminum powder paste, powder material and slurry; the formula comprises the aluminum powder paste, the powder material and the slurry in parts by mass: 0.075 to 0.085 part of the aluminum powder paste, 25 to 35 parts of the powder material and 65 to 75 parts of the slurry; the powder material comprises cement, waste concrete powder, waste brick powder, composite fiber powder and a mothproof agent in parts by mass: 25-38 parts of cement, 12-20 parts of waste concrete powder, 12-22 parts of waste brick powder, 25-50 parts of composite fiber powder and 0.5-1.5 parts of the mothproof agent. The slurry is formed by mixing and grinding quartz sand tailings, silt, waste gypsum, shells, eggshells and water and comprises 5-20 parts of quartz sand tailings, 5-15 parts of silt, 7-15 parts of waste gypsum, 5-17 parts of the shells, 7-20 parts of the eggshells and 51-57 parts of water. The anti-cracking, anti-compression, anti-impact, anti-seepage, anti-crushing and heat-insulating properties of the autoclaved aerated concrete block are improved, so that the conservation of building construction and the energy conservation of buildings are promoted.
一种蒸压加气混凝土砌块配方,包括铝粉膏、粉料、浆料;所述铝粉膏、粉料、浆料的质量份配比为:铝粉膏0.075‑0.085份、粉料25‑35份、浆料65‑75份;所述粉料的组成包括水泥、废混凝土粉、废砖粉、复合纤维粉、防蛀剂;其质量份配比为:水泥25‑38份;废混凝土粉12‑20份、废砖粉12‑22份、复合纤维粉25‑50份、防蛀剂0.5‑1.5份;所述浆料由石英砂尾矿、淤沙、废石膏、贝壳、蛋壳与水混合研磨而成;所述浆料的石英砂尾矿5‑20份、淤沙5‑15份、废石膏7‑15份、贝壳5‑17份、蛋壳7‑20份、水51‑57份;提高蒸压加气混凝土砌块的抗裂、抗压、抗冲击、防渗、抗碎、保温的性能,从而促进了建筑施工的节约与建筑物的节能。
Formula of autoclaved aerated concrete block
The formula of an autoclaved aerated concrete block comprises aluminum powder paste, powder material and slurry; the formula comprises the aluminum powder paste, the powder material and the slurry in parts by mass: 0.075 to 0.085 part of the aluminum powder paste, 25 to 35 parts of the powder material and 65 to 75 parts of the slurry; the powder material comprises cement, waste concrete powder, waste brick powder, composite fiber powder and a mothproof agent in parts by mass: 25-38 parts of cement, 12-20 parts of waste concrete powder, 12-22 parts of waste brick powder, 25-50 parts of composite fiber powder and 0.5-1.5 parts of the mothproof agent. The slurry is formed by mixing and grinding quartz sand tailings, silt, waste gypsum, shells, eggshells and water and comprises 5-20 parts of quartz sand tailings, 5-15 parts of silt, 7-15 parts of waste gypsum, 5-17 parts of the shells, 7-20 parts of the eggshells and 51-57 parts of water. The anti-cracking, anti-compression, anti-impact, anti-seepage, anti-crushing and heat-insulating properties of the autoclaved aerated concrete block are improved, so that the conservation of building construction and the energy conservation of buildings are promoted.
一种蒸压加气混凝土砌块配方,包括铝粉膏、粉料、浆料;所述铝粉膏、粉料、浆料的质量份配比为:铝粉膏0.075‑0.085份、粉料25‑35份、浆料65‑75份;所述粉料的组成包括水泥、废混凝土粉、废砖粉、复合纤维粉、防蛀剂;其质量份配比为:水泥25‑38份;废混凝土粉12‑20份、废砖粉12‑22份、复合纤维粉25‑50份、防蛀剂0.5‑1.5份;所述浆料由石英砂尾矿、淤沙、废石膏、贝壳、蛋壳与水混合研磨而成;所述浆料的石英砂尾矿5‑20份、淤沙5‑15份、废石膏7‑15份、贝壳5‑17份、蛋壳7‑20份、水51‑57份;提高蒸压加气混凝土砌块的抗裂、抗压、抗冲击、防渗、抗碎、保温的性能,从而促进了建筑施工的节约与建筑物的节能。
Formula of autoclaved aerated concrete block
一种蒸压加气混凝土砌块配方
CHEN KUNZHONG (author)
2021-09-14
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Autoclaved aerated concrete block production method and autoclaved aerated concrete block
European Patent Office | 2021
|Preparation method of autoclaved aerated concrete block and autoclaved aerated concrete block
European Patent Office | 2021
|European Patent Office | 2023
|