A platform for research: civil engineering, architecture and urbanism
The invention discloses a sludge pressed brick formula in the technical field of building material processing. The sludge pressed brick formula comprises the following components: 40-60% of a base material; 20%-30% of aggregate; 10%-20% of auxiliary materials; and 2%-5% of a curing agent. According to the sludge pressed brick formula, the base material and the aggregate are combined and matched, the auxiliary materials are added after the curing agent is stirred, the mixture is aired, and the proportion of the formula is adjusted, so that a finished product can conveniently form a smooth surface, the attractiveness is improved, the protrusion feeling of impurities is obviously reduced, the size is convenient to control, meanwhile, the internal combination sealing performance is improved, and the toughness of an inner core is higher; and meanwhile, crushed construction waste is added into the aggregate and is combined with the sludge, so that a positive effect is effectively achieved on river channel engineering dredging, the recycling rate of waste is high, energy is saved, environment friendliness is achieved, the strength of a finished product is improved, and the application range is wide.
本发明公开了建筑材料加工技术领域的一种淤泥压砖配方,该种淤泥压砖配方组成为:基料:40%~60%;骨料:20%~30%;辅料:10%~20%;固化剂:2%~5%,该种淤泥压砖配方,通过基料、骨料的组合配合,并在固化剂搅拌后进行辅料的添加,并晾晒,调整配比配方的比例,便于使成品形成光面,美观度提升,杂质凸出感明显减少,便于尺寸控制的同时,内部组合密封性提升,内芯韧性更强,减少断坯率,降低损耗,同时在骨料中添加建筑垃圾粉碎物并配合淤泥组合,有效的对河道工程疏浚起到积极作用,废物循环利用率高,节能环保,且成品强度提升,适用范围广。
The invention discloses a sludge pressed brick formula in the technical field of building material processing. The sludge pressed brick formula comprises the following components: 40-60% of a base material; 20%-30% of aggregate; 10%-20% of auxiliary materials; and 2%-5% of a curing agent. According to the sludge pressed brick formula, the base material and the aggregate are combined and matched, the auxiliary materials are added after the curing agent is stirred, the mixture is aired, and the proportion of the formula is adjusted, so that a finished product can conveniently form a smooth surface, the attractiveness is improved, the protrusion feeling of impurities is obviously reduced, the size is convenient to control, meanwhile, the internal combination sealing performance is improved, and the toughness of an inner core is higher; and meanwhile, crushed construction waste is added into the aggregate and is combined with the sludge, so that a positive effect is effectively achieved on river channel engineering dredging, the recycling rate of waste is high, energy is saved, environment friendliness is achieved, the strength of a finished product is improved, and the application range is wide.
本发明公开了建筑材料加工技术领域的一种淤泥压砖配方,该种淤泥压砖配方组成为:基料:40%~60%;骨料:20%~30%;辅料:10%~20%;固化剂:2%~5%,该种淤泥压砖配方,通过基料、骨料的组合配合,并在固化剂搅拌后进行辅料的添加,并晾晒,调整配比配方的比例,便于使成品形成光面,美观度提升,杂质凸出感明显减少,便于尺寸控制的同时,内部组合密封性提升,内芯韧性更强,减少断坯率,降低损耗,同时在骨料中添加建筑垃圾粉碎物并配合淤泥组合,有效的对河道工程疏浚起到积极作用,废物循环利用率高,节能环保,且成品强度提升,适用范围广。
Sludge pressed brick formula
一种淤泥压砖配方
ZHOU BINSHENG (author)
2021-10-12
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
High-strength environment-friendly composite pressed brick formula
European Patent Office | 2021
|Municipal sludge coal gangue hollow brick formula and production method
European Patent Office | 2020
|Brick making formula based on dredged sludge, process and application
European Patent Office | 2023