Continuous carbon fiber reinforced phosphoric acid-based geopolymer composite material and preparation method thereof
The invention discloses a continuous carbon fiber reinforced phosphoric acid-based geopolymer composite material and a preparation method thereof. The preparation method comprises the following steps: vacuum heat treatment on carbon fibers; activation pretreatment of an aluminum-silicon source: calcining the superfine kaolin powder to prepare metakaolin powder; diluting concentrated phosphoric acid into a phosphoric acid solution; and uniformly mixing the metakaolin powder with a phosphoric acid solution to prepare phosphoric acid-based geopolymer slurry; preparation and pretreatent of a mold; forming of the continuous carbon fiber reinforced phosphoric acid-based geopolymer composite material: uniformly printing the slurry on pretreated carbon fibers in a screen printing manner, and then stacking the carbon fibers on a prefabricated mold layer by layer to form a rough blank; curing, demolding and curing; and silicon resin solution surface treatment. The prepared composite material is composed of a phosphoric acid-based geopolymer and continuous carbon fibers uniformly distributed in the phosphoric acid-based geopolymer. The composite material is excellent in mechanical property and outstanding in high and low temperature resistance, and the preparation method is low in energy consumption and cost and simple in process.
本发明公开了一种连续碳纤维增强磷酸基地质聚合物复合材料及其制备方法,制备方法包括:碳纤维的真空热处理;铝‑硅源的活化前处理:将超细高岭土粉末煅烧制得偏高岭土粉末;将浓磷酸稀释为磷酸溶液;将偏高岭土粉末与磷酸溶液混匀制得磷酸基地质聚合物浆料;模具的准备与预处理;连续碳纤维增强磷酸基地质聚合物复合材料的成型:通过丝网印刷方式将浆料均匀印刷在预处理后的碳纤维上,随后逐层叠放至预制好的模具上,形成粗坯;固化与脱模养护;硅树脂溶液表面处理。制得的复合材料由磷酸基地质聚合物和均匀分布于磷酸基地质聚合物中的连续碳纤维构成。本发明的复合材料力学性能优良、耐高低温性能突出,制备方法能耗成本低、工艺简单。
Continuous carbon fiber reinforced phosphoric acid-based geopolymer composite material and preparation method thereof
The invention discloses a continuous carbon fiber reinforced phosphoric acid-based geopolymer composite material and a preparation method thereof. The preparation method comprises the following steps: vacuum heat treatment on carbon fibers; activation pretreatment of an aluminum-silicon source: calcining the superfine kaolin powder to prepare metakaolin powder; diluting concentrated phosphoric acid into a phosphoric acid solution; and uniformly mixing the metakaolin powder with a phosphoric acid solution to prepare phosphoric acid-based geopolymer slurry; preparation and pretreatent of a mold; forming of the continuous carbon fiber reinforced phosphoric acid-based geopolymer composite material: uniformly printing the slurry on pretreated carbon fibers in a screen printing manner, and then stacking the carbon fibers on a prefabricated mold layer by layer to form a rough blank; curing, demolding and curing; and silicon resin solution surface treatment. The prepared composite material is composed of a phosphoric acid-based geopolymer and continuous carbon fibers uniformly distributed in the phosphoric acid-based geopolymer. The composite material is excellent in mechanical property and outstanding in high and low temperature resistance, and the preparation method is low in energy consumption and cost and simple in process.
本发明公开了一种连续碳纤维增强磷酸基地质聚合物复合材料及其制备方法,制备方法包括:碳纤维的真空热处理;铝‑硅源的活化前处理:将超细高岭土粉末煅烧制得偏高岭土粉末;将浓磷酸稀释为磷酸溶液;将偏高岭土粉末与磷酸溶液混匀制得磷酸基地质聚合物浆料;模具的准备与预处理;连续碳纤维增强磷酸基地质聚合物复合材料的成型:通过丝网印刷方式将浆料均匀印刷在预处理后的碳纤维上,随后逐层叠放至预制好的模具上,形成粗坯;固化与脱模养护;硅树脂溶液表面处理。制得的复合材料由磷酸基地质聚合物和均匀分布于磷酸基地质聚合物中的连续碳纤维构成。本发明的复合材料力学性能优良、耐高低温性能突出,制备方法能耗成本低、工艺简单。
Continuous carbon fiber reinforced phosphoric acid-based geopolymer composite material and preparation method thereof
连续碳纤维增强磷酸基地质聚合物复合材料及其制备方法
HE MIN (author) / YANG ZONGBAO (author) / YANG QINGGUANG (author)
2021-12-17
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2021
|Basalt fiber reinforced geopolymer composite grouting material and preparation method thereof
European Patent Office | 2020
|Granite stone powder phosphoric acid-based geopolymer and preparation method thereof
European Patent Office | 2024
|Phosphoric acid-based geopolymer semi-rigid base material and application thereof
European Patent Office | 2023
|European Patent Office | 2022
|