A platform for research: civil engineering, architecture and urbanism
Production process of ceramic tile wallboard matched with integral bathroom
The invention discloses a production process of a ceramic tile wallboard matched with a whole bathroom. The production process comprises the following steps: step 1, manufacturing a wallboard framework; 2, ceramic tile cutting; step 3, splicing the wall plates; 4, wall plate filling; fifthly, pressure maintaining and curing are conducted; step 6, demolding the wallboard; step 7, detecting and storing; wherein in the first step, firstly, an alloy block is placed in a smelting furnace, the temperature of the interior of the alloy block is increased to 1200-1600 DEG C, the heating time is 1-3 h, during smelting, a specific wall plate framework mold is manufactured, after smelting is finished, molten alloy is injected into the mold, then air cooling is conducted, after a wall plate framework is cooled and formed, dust on the wall plate framework is cleared away, and the wall plate framework is put into the smelting furnace; then, redundant parts are polished away; according to the method, the appropriate wall plate can be made according to the characteristics of the ceramic tile, the production time can be shortened, manpower, material resources and raw materials can be saved, the production efficiency and the safety effect can be improved, the process is simple, and manufacturing is convenient.
本发明公开了一种整体卫浴配套的瓷砖壁板生产工艺,包括以下步骤:步骤一,制作壁板骨架;步骤二,瓷砖切割;步骤三,壁板拼接;步骤四,壁板填充;步骤五,保压固化;步骤六,壁板脱模;步骤七,检测储存;其中在上述步骤一中,首先将合金块放到熔炉内部,将其内部的温度加热到1200‑1600℃,加热时间为1‑3h,在熔化时,制作特定的壁板骨架模具,在熔化结束后,将熔融态的合金注入模具内部,然后进行空冷,当壁板骨架冷却成型后,将上面的灰尘进行清理,然后打磨掉多余的部分;该发明能够按照瓷砖的特点进行制定较合适的壁板,可以减少生产时间,不仅能节省人力、物力与原材料,还能提高生产效率和安全效果,而且工艺简单,方便制作。
Production process of ceramic tile wallboard matched with integral bathroom
The invention discloses a production process of a ceramic tile wallboard matched with a whole bathroom. The production process comprises the following steps: step 1, manufacturing a wallboard framework; 2, ceramic tile cutting; step 3, splicing the wall plates; 4, wall plate filling; fifthly, pressure maintaining and curing are conducted; step 6, demolding the wallboard; step 7, detecting and storing; wherein in the first step, firstly, an alloy block is placed in a smelting furnace, the temperature of the interior of the alloy block is increased to 1200-1600 DEG C, the heating time is 1-3 h, during smelting, a specific wall plate framework mold is manufactured, after smelting is finished, molten alloy is injected into the mold, then air cooling is conducted, after a wall plate framework is cooled and formed, dust on the wall plate framework is cleared away, and the wall plate framework is put into the smelting furnace; then, redundant parts are polished away; according to the method, the appropriate wall plate can be made according to the characteristics of the ceramic tile, the production time can be shortened, manpower, material resources and raw materials can be saved, the production efficiency and the safety effect can be improved, the process is simple, and manufacturing is convenient.
本发明公开了一种整体卫浴配套的瓷砖壁板生产工艺,包括以下步骤:步骤一,制作壁板骨架;步骤二,瓷砖切割;步骤三,壁板拼接;步骤四,壁板填充;步骤五,保压固化;步骤六,壁板脱模;步骤七,检测储存;其中在上述步骤一中,首先将合金块放到熔炉内部,将其内部的温度加热到1200‑1600℃,加热时间为1‑3h,在熔化时,制作特定的壁板骨架模具,在熔化结束后,将熔融态的合金注入模具内部,然后进行空冷,当壁板骨架冷却成型后,将上面的灰尘进行清理,然后打磨掉多余的部分;该发明能够按照瓷砖的特点进行制定较合适的壁板,可以减少生产时间,不仅能节省人力、物力与原材料,还能提高生产效率和安全效果,而且工艺简单,方便制作。
Production process of ceramic tile wallboard matched with integral bathroom
一种整体卫浴配套的瓷砖壁板生产工艺
TANG TAIYING (author)
2022-03-18
Patent
Electronic Resource
Chinese
Wallboard unit, manufacturing method of wallboard unit, bathroom wall surface and integral bathroom
European Patent Office | 2022
|External corner splicing structure for integral bathroom wallboard
European Patent Office | 2023
|Internal corner splicing structure for integral bathroom wallboard
European Patent Office | 2023
|