Autoclaved aerated concrete anti-seepage building block and preparation method thereof
The invention discloses an autoclaved aerated concrete anti-seepage building block and a preparation method thereof, the autoclaved aerated concrete anti-seepage building block takes finely ground quartz sand, cement, lime and gypsum as main base materials and aluminum powder as a foaming agent, and the autoclaved aerated concrete anti-seepage building block is characterized by comprising a hydrophobic anti-seepage agent, and the addition amount of the hydrophobic anti-seepage agent is 0.03-0.05% of the total amount by weight. The method comprises the following steps: mixing the components, stirring, standing, cutting, and curing for 10-12 hours at the high temperature of 180-200 DEG C and the high pressure of 10-12 standard atmospheric pressure to prepare the autoclaved aerated concrete anti-seepage building block. The invention relates to a sand aerated impervious concrete wall which has an impervious function and can not meet the waterproof and impervious requirements of a building in the existing sand aerated concrete wall.
本发明公开了一种蒸压加气混凝土防渗砌块及其的制备方法,包括以磨细石英砂、水泥、石灰、石膏为主要基材,以铝粉为发泡剂,其特征在于:包括憎水性防渗剂,其加入量按重量百分比计为总量的0.03~0.05%。其方法步骤为:将各组分经混合配料、搅拌、静停、切割,在高温180~200℃,高压10~12个标准大气压下养护10~12小时制成蒸压加气混凝土防渗砌块。本发明对现有砂加气混凝土墙体本身不能达到建筑防水抗渗要求的,具有防渗功能的砂加气防渗混凝土墙体。
Autoclaved aerated concrete anti-seepage building block and preparation method thereof
The invention discloses an autoclaved aerated concrete anti-seepage building block and a preparation method thereof, the autoclaved aerated concrete anti-seepage building block takes finely ground quartz sand, cement, lime and gypsum as main base materials and aluminum powder as a foaming agent, and the autoclaved aerated concrete anti-seepage building block is characterized by comprising a hydrophobic anti-seepage agent, and the addition amount of the hydrophobic anti-seepage agent is 0.03-0.05% of the total amount by weight. The method comprises the following steps: mixing the components, stirring, standing, cutting, and curing for 10-12 hours at the high temperature of 180-200 DEG C and the high pressure of 10-12 standard atmospheric pressure to prepare the autoclaved aerated concrete anti-seepage building block. The invention relates to a sand aerated impervious concrete wall which has an impervious function and can not meet the waterproof and impervious requirements of a building in the existing sand aerated concrete wall.
本发明公开了一种蒸压加气混凝土防渗砌块及其的制备方法,包括以磨细石英砂、水泥、石灰、石膏为主要基材,以铝粉为发泡剂,其特征在于:包括憎水性防渗剂,其加入量按重量百分比计为总量的0.03~0.05%。其方法步骤为:将各组分经混合配料、搅拌、静停、切割,在高温180~200℃,高压10~12个标准大气压下养护10~12小时制成蒸压加气混凝土防渗砌块。本发明对现有砂加气混凝土墙体本身不能达到建筑防水抗渗要求的,具有防渗功能的砂加气防渗混凝土墙体。
Autoclaved aerated concrete anti-seepage building block and preparation method thereof
一种蒸压加气混凝土防渗砌块及其的制备方法
CHEN HAIMING (author) / KONG ZUOFAN (author) / LU WEIDONG (author) / DENG QINGSONG (author) / ZHANG BO (author) / LU JUNHUA (author) / GU XINGKUN (author)
2022-04-12
Patent
Electronic Resource
Chinese
Preparation method of autoclaved aerated concrete block and autoclaved aerated concrete block
European Patent Office | 2021
|European Patent Office | 2016
|Autoclaved aerated concrete building block and preparation method thereof
European Patent Office | 2015
|European Patent Office | 2023
|Autoclaved aerated concrete block production method and autoclaved aerated concrete block
European Patent Office | 2021
|