Anti-radiation green brick, anti-radiation brick and preparation method thereof
The invention provides an anti-radiation green brick, an anti-radiation brick and a preparation method thereof. The raw materials of the radiation-proof green brick comprise powder and an additive, wherein the powder material comprises the following components in percentage by mass: 24%-26% of barium sulfate of 9-16 meshes, 24%-26% of barium sulfate of 20-25 meshes, 16%-18% of barium sulfate of 80-90 meshes, 16%-18% of barium sulfate of 320-330 meshes and 16%-18% of cement; the additives comprise phenolic resin, a binder and a diluent. The preparation method of the anti-radiation green brick comprises the following steps: mixing and pressing the raw materials to obtain the anti-radiation green brick. The invention further provides an anti-radiation brick. The anti-radiation brick comprises the anti-radiation green brick. The preparation method of the anti-radiation brick comprises the following steps: glazing the surface of the anti-radiation brick blank, and firing to obtain the anti-radiation brick. The anti-radiation brick provided by the invention is high in anti-radiation strength and excellent in breaking strength, wear resistance, oil stain resistance, corrosion resistance and the like.
本申请提供了一种防辐射砖坯、防辐射砖及其制备方法。该防辐射砖坯原料包括粉料和添加剂;其中,粉料按质量百分比计,包括:9~16目硫酸钡24%~26%、20~25目硫酸钡24%~26%、80~90目硫酸钡16%~18%、320~330目硫酸钡16%~18%和水泥16%~18%;添加剂包括酚醛树脂、粘结剂和稀释剂。该防辐射砖坯的制备方法是将上述原料混合,压制,得到防辐射砖坯。本申请还提供了一种防辐射砖,包括上述的防辐射砖坯;该防辐射砖的制备方法包括:在所述防辐射砖坯表面上釉,烧成,得到防辐射砖。本申请提供的防辐射砖,防辐射强度高,且抗折强度、耐磨性能、耐油污、耐腐蚀等性能优异。
Anti-radiation green brick, anti-radiation brick and preparation method thereof
The invention provides an anti-radiation green brick, an anti-radiation brick and a preparation method thereof. The raw materials of the radiation-proof green brick comprise powder and an additive, wherein the powder material comprises the following components in percentage by mass: 24%-26% of barium sulfate of 9-16 meshes, 24%-26% of barium sulfate of 20-25 meshes, 16%-18% of barium sulfate of 80-90 meshes, 16%-18% of barium sulfate of 320-330 meshes and 16%-18% of cement; the additives comprise phenolic resin, a binder and a diluent. The preparation method of the anti-radiation green brick comprises the following steps: mixing and pressing the raw materials to obtain the anti-radiation green brick. The invention further provides an anti-radiation brick. The anti-radiation brick comprises the anti-radiation green brick. The preparation method of the anti-radiation brick comprises the following steps: glazing the surface of the anti-radiation brick blank, and firing to obtain the anti-radiation brick. The anti-radiation brick provided by the invention is high in anti-radiation strength and excellent in breaking strength, wear resistance, oil stain resistance, corrosion resistance and the like.
本申请提供了一种防辐射砖坯、防辐射砖及其制备方法。该防辐射砖坯原料包括粉料和添加剂;其中,粉料按质量百分比计,包括:9~16目硫酸钡24%~26%、20~25目硫酸钡24%~26%、80~90目硫酸钡16%~18%、320~330目硫酸钡16%~18%和水泥16%~18%;添加剂包括酚醛树脂、粘结剂和稀释剂。该防辐射砖坯的制备方法是将上述原料混合,压制,得到防辐射砖坯。本申请还提供了一种防辐射砖,包括上述的防辐射砖坯;该防辐射砖的制备方法包括:在所述防辐射砖坯表面上釉,烧成,得到防辐射砖。本申请提供的防辐射砖,防辐射强度高,且抗折强度、耐磨性能、耐油污、耐腐蚀等性能优异。
Anti-radiation green brick, anti-radiation brick and preparation method thereof
一种防辐射砖坯、防辐射砖及其制备方法
LIU YINGYING (author) / LIU JUNRONG (author)
2022-04-15
Patent
Electronic Resource
Chinese
Anti-cracking perforated brick and preparation method thereof
European Patent Office | 2022
|Anti-distortion magnesia carbon brick and preparation method thereof
European Patent Office | 2024
|Anti-freezing fly ash brick and preparation method thereof
European Patent Office | 2021
|European Patent Office | 2021
|