Corrosion-resistant ceramic formula and ceramic vase
The embodiment of the invention provides a corrosion-resistant ceramic formula and a ceramic vase. The corrosion-resistant ceramic formula is prepared from the following raw materials in parts by weight: 50-70 parts of ceramic polishing waste, 20-26 parts of nano calcium carbonate, 13-18 parts of jade powder, 8-17 parts of volcanic rock, 3-10 parts of silicified graphite, 35-55 parts of zirconite, 3-8 parts of knar clay, 1-3 parts of tricalcium phosphate, 2.5-3.6 parts of nano magnesium oxide and 8-11 parts of blast furnace slag. According to the embodiment of the invention, the ceramic material prepared from the ceramic polishing waste, the nano calcium carbonate, the volcanic rock, the zirconite, the knar clay, the nano magnesium oxide, the blast furnace slag and the like has relatively good corrosion resistance, and the corrosion resistance of the ceramic material is further enhanced through matched use of the silicified graphite; and the produced ceramic material is good in corrosion resistance and long in service life.
本申请实施例提供了一种耐腐蚀陶瓷配方及陶瓷花瓶,所述耐腐蚀陶瓷配方由以下重量份原料制成:陶瓷抛光废料50~70份、纳米碳酸钙20~26份、玉石粉13~18份、火山岩8~17份、硅化石墨3~10份、锆英石35~55份、木节粘土3~8份、磷酸三钙1~3份、纳米氧化镁2.5~3.6份、高炉矿渣8~11份。本申请实施例通过陶瓷抛光废料、纳米碳酸钙、火山岩、锆英石、木节粘土、纳米氧化镁以及高炉矿渣等制得的陶瓷材料具有较好的耐腐蚀性能,通过采用硅化石墨的配合使用进一步增强了陶瓷材料的耐腐蚀性能,生产出的陶瓷材料耐腐蚀性能好,使用寿命长。
Corrosion-resistant ceramic formula and ceramic vase
The embodiment of the invention provides a corrosion-resistant ceramic formula and a ceramic vase. The corrosion-resistant ceramic formula is prepared from the following raw materials in parts by weight: 50-70 parts of ceramic polishing waste, 20-26 parts of nano calcium carbonate, 13-18 parts of jade powder, 8-17 parts of volcanic rock, 3-10 parts of silicified graphite, 35-55 parts of zirconite, 3-8 parts of knar clay, 1-3 parts of tricalcium phosphate, 2.5-3.6 parts of nano magnesium oxide and 8-11 parts of blast furnace slag. According to the embodiment of the invention, the ceramic material prepared from the ceramic polishing waste, the nano calcium carbonate, the volcanic rock, the zirconite, the knar clay, the nano magnesium oxide, the blast furnace slag and the like has relatively good corrosion resistance, and the corrosion resistance of the ceramic material is further enhanced through matched use of the silicified graphite; and the produced ceramic material is good in corrosion resistance and long in service life.
本申请实施例提供了一种耐腐蚀陶瓷配方及陶瓷花瓶,所述耐腐蚀陶瓷配方由以下重量份原料制成:陶瓷抛光废料50~70份、纳米碳酸钙20~26份、玉石粉13~18份、火山岩8~17份、硅化石墨3~10份、锆英石35~55份、木节粘土3~8份、磷酸三钙1~3份、纳米氧化镁2.5~3.6份、高炉矿渣8~11份。本申请实施例通过陶瓷抛光废料、纳米碳酸钙、火山岩、锆英石、木节粘土、纳米氧化镁以及高炉矿渣等制得的陶瓷材料具有较好的耐腐蚀性能,通过采用硅化石墨的配合使用进一步增强了陶瓷材料的耐腐蚀性能,生产出的陶瓷材料耐腐蚀性能好,使用寿命长。
Corrosion-resistant ceramic formula and ceramic vase
一种耐腐蚀陶瓷配方及陶瓷花瓶
SU CHENYI (author) / SU YAOZHENG (author) / LIU WENJIAN (author)
2022-04-19
Patent
Electronic Resource
Chinese
Corrosion-resistant ceramic formula and preparation method of ceramic product
European Patent Office | 2024
|Corrosion-resistant ceramic formula and preparation method of ceramic product
European Patent Office | 2021
|