High-strength low-expansion-coefficient glass fiber and composite material
The invention provides a high-strength and low-expansion-coefficient glass fiber which comprises the following components in percentage by mass: 60-66.5% of SiO2; 18% to 22% of Al2O3; 0 to 3.0% of CaO; 10 to 15% of MgO; 0.3% to 3% of P2O5; 0% to 0.9% of Na2O + K2O; 0 to 0.6 percent of Fe2O3 (ferric oxide); 0.4 to 2 percent of TiO2; 0.2% to 3% of Y2O3; the content of each component is in percentage by mass, the sum of the content of SiO2 and the content of P2O5 is 61.4-68%, the sum of the content of TiO2 and the content of Y2O3 is 1-4.5%, and the ratio of the content of Y2O3 to the content of TiO2 is 0.1-7.5. The high-strength and low-expansion-coefficient glass fiber provided by the invention is easy to wire-draw and form, and has relatively high strength and relatively low expansion coefficient.
本发明提供一种高强度、低膨胀系数玻璃纤维,包括以下成分,各成分的含量为质量百分比:60‑66.5%的SiO2;18‑22%的Al2O3;0‑3.0%的CaO;10‑15%的MgO;0.3‑3%的P2O5;0‑0.9%的Na2O+K2O;0‑0.6%的Fe2O3;0.4‑2%的TiO2;0.2‑3%的Y2O3;各成分的含量为质量百分比,并且SiO2含量与P2O5含量之和为61.4‑68%,TiO2含量与Y2O3含量之和为1‑4.5%,Y2O3含量/TiO2含量为0.1‑7.5。本发明提供的高强度、低膨胀系数玻璃纤维,易于拉丝成形,且具有较高的强度和较低的膨胀系数。
High-strength low-expansion-coefficient glass fiber and composite material
The invention provides a high-strength and low-expansion-coefficient glass fiber which comprises the following components in percentage by mass: 60-66.5% of SiO2; 18% to 22% of Al2O3; 0 to 3.0% of CaO; 10 to 15% of MgO; 0.3% to 3% of P2O5; 0% to 0.9% of Na2O + K2O; 0 to 0.6 percent of Fe2O3 (ferric oxide); 0.4 to 2 percent of TiO2; 0.2% to 3% of Y2O3; the content of each component is in percentage by mass, the sum of the content of SiO2 and the content of P2O5 is 61.4-68%, the sum of the content of TiO2 and the content of Y2O3 is 1-4.5%, and the ratio of the content of Y2O3 to the content of TiO2 is 0.1-7.5. The high-strength and low-expansion-coefficient glass fiber provided by the invention is easy to wire-draw and form, and has relatively high strength and relatively low expansion coefficient.
本发明提供一种高强度、低膨胀系数玻璃纤维,包括以下成分,各成分的含量为质量百分比:60‑66.5%的SiO2;18‑22%的Al2O3;0‑3.0%的CaO;10‑15%的MgO;0.3‑3%的P2O5;0‑0.9%的Na2O+K2O;0‑0.6%的Fe2O3;0.4‑2%的TiO2;0.2‑3%的Y2O3;各成分的含量为质量百分比,并且SiO2含量与P2O5含量之和为61.4‑68%,TiO2含量与Y2O3含量之和为1‑4.5%,Y2O3含量/TiO2含量为0.1‑7.5。本发明提供的高强度、低膨胀系数玻璃纤维,易于拉丝成形,且具有较高的强度和较低的膨胀系数。
High-strength low-expansion-coefficient glass fiber and composite material
高强度、低膨胀系数玻璃纤维及复合材料
HAN LIXIONG (author) / ZENG QINGWEN (author) / TAN JIADING (author) / HOU QINGFENG (author) / SONG FAN (author) / FENG JIACHENG (author) / XU QIANG (author) / FAN ZHENHUA (author) / ZHAO SHIBIN (author) / ZHANG CONG (author)
2022-05-27
Patent
Electronic Resource
Chinese
High-strength glass fiber composite material and preparation method thereof
European Patent Office | 2020
|High-strength composite ceramic based on high-temperature thermal expansion coefficient matching
European Patent Office | 2024
|