The invention discloses energy-saving and environment-friendly building cement, which is prepared from the following ingredients in parts by weight: 150 to 180 parts of limestone, 50 to 60 parts of coal ash, 8 to 10 parts of copper slag, 15 to 20 parts of kaolin, 20 to 30 parts of sandstone, 5 to 8 parts of aluminum oxide, 5 to 8 parts of wood calcium, 6 to 8 parts of iron-ore slag and 8 to 10 parts of straw. Wherein the particle size of the straw is 120-200 meshes. According to the energy-saving and environment-friendly building cement provided by the invention, the industrial waste residues are recycled, and the strength of the cement is improved.
本发明公开了一种节能环保型建筑水泥,包括按重量份数计的如下成分:石灰石150‑180份、粉煤灰50‑60份、铜矿渣8‑10份、高岭土15‑20份、砂岩20‑30份、氧化铝5‑8份、木质钙5‑8份、铁矿渣6‑8份、秸秆8‑10份;其中秸秆的粒径为120‑200目。本发明提供的节能环保型建筑水泥,对工业废渣进行了再利用,并提高了水泥的强度。
The invention discloses energy-saving and environment-friendly building cement, which is prepared from the following ingredients in parts by weight: 150 to 180 parts of limestone, 50 to 60 parts of coal ash, 8 to 10 parts of copper slag, 15 to 20 parts of kaolin, 20 to 30 parts of sandstone, 5 to 8 parts of aluminum oxide, 5 to 8 parts of wood calcium, 6 to 8 parts of iron-ore slag and 8 to 10 parts of straw. Wherein the particle size of the straw is 120-200 meshes. According to the energy-saving and environment-friendly building cement provided by the invention, the industrial waste residues are recycled, and the strength of the cement is improved.
本发明公开了一种节能环保型建筑水泥,包括按重量份数计的如下成分:石灰石150‑180份、粉煤灰50‑60份、铜矿渣8‑10份、高岭土15‑20份、砂岩20‑30份、氧化铝5‑8份、木质钙5‑8份、铁矿渣6‑8份、秸秆8‑10份;其中秸秆的粒径为120‑200目。本发明提供的节能环保型建筑水泥,对工业废渣进行了再利用,并提高了水泥的强度。
Energy-saving and environment-friendly building cement and production process thereof