A platform for research: civil engineering, architecture and urbanism
Two-component ceramic tile back adhesive and preparation method thereof
The invention provides a two-component ceramic tile back adhesive, which comprises a liquid material component A and a powder material component B. The weight ratio of the liquid material component A to the powder material component B is 1: 1.5-2, the liquid material component A comprises the following raw materials in parts by weight: 70-140 parts of emulsion, 1-6 parts of a waterproof agent and 2-6 parts of an auxiliary agent I, and the powder material component B comprises the following raw materials in parts by weight: 35-55 parts of white cement and 35-55 parts of fine sand. 1-10 parts of konjac powder and 1-3 parts of an auxiliary agent II. In addition, the invention further provides a preparation method of the two-component ceramic tile back adhesive, and the preparation method comprises the following steps: mixing the liquid material component and the powder material component. The double-component ceramic tile back adhesive provided by the invention not only has better water resistance and aging resistance, but also has little change in characteristics after freeze-thaw cycle.
本发明提供了双组份瓷砖背胶,包括液料组份A和粉料组份B,所述液料组份A和粉料组份B的重量比为1:1.5~2,按重量份数计,所述液料组份A的原料组成包括:乳液70~140份,防水剂1~6份,助剂一2~6份,按重量份数计,所述粉料组份B的原料组成包括:白水泥35~55份,细砂35~55份,魔芋精粉1~10份,助剂二1~3份。此外,本发明还提提供了一种双组分瓷砖背胶制备方法,包括如下步骤:将液料组份和粉料组份进行混合。本发明所提供的双组分瓷砖背胶,不仅具有较好的耐水和耐老化性能,且冻融循环后的特性改变不大。
Two-component ceramic tile back adhesive and preparation method thereof
The invention provides a two-component ceramic tile back adhesive, which comprises a liquid material component A and a powder material component B. The weight ratio of the liquid material component A to the powder material component B is 1: 1.5-2, the liquid material component A comprises the following raw materials in parts by weight: 70-140 parts of emulsion, 1-6 parts of a waterproof agent and 2-6 parts of an auxiliary agent I, and the powder material component B comprises the following raw materials in parts by weight: 35-55 parts of white cement and 35-55 parts of fine sand. 1-10 parts of konjac powder and 1-3 parts of an auxiliary agent II. In addition, the invention further provides a preparation method of the two-component ceramic tile back adhesive, and the preparation method comprises the following steps: mixing the liquid material component and the powder material component. The double-component ceramic tile back adhesive provided by the invention not only has better water resistance and aging resistance, but also has little change in characteristics after freeze-thaw cycle.
本发明提供了双组份瓷砖背胶,包括液料组份A和粉料组份B,所述液料组份A和粉料组份B的重量比为1:1.5~2,按重量份数计,所述液料组份A的原料组成包括:乳液70~140份,防水剂1~6份,助剂一2~6份,按重量份数计,所述粉料组份B的原料组成包括:白水泥35~55份,细砂35~55份,魔芋精粉1~10份,助剂二1~3份。此外,本发明还提提供了一种双组分瓷砖背胶制备方法,包括如下步骤:将液料组份和粉料组份进行混合。本发明所提供的双组分瓷砖背胶,不仅具有较好的耐水和耐老化性能,且冻融循环后的特性改变不大。
Two-component ceramic tile back adhesive and preparation method thereof
一种双组份瓷砖背胶及其制备方法
CHEN LEZHOU (author)
2022-06-07
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Two-component ceramic tile back adhesive and preparation method thereof
European Patent Office | 2023
|Double-component water-based ceramic tile back adhesive and preparation method thereof
European Patent Office | 2020
|Super-water-resistant two-component ceramic tile back adhesive and preparation method thereof
European Patent Office | 2024
|European Patent Office | 2022
|