Color-adjustable light storage ceramic and preparation method thereof
The invention is applicable to the field of light-storing ceramics, and provides a color-adjustable light-storing ceramic and a preparation method thereof.The method comprises the steps that S01, weighing is conducted, specifically, 35%-44% by mass of 10-30-mesh quartz raw materials, 35%-40% by mass of 50-100-mesh quartz raw materials, 5%-15% by mass of 150-250-mesh quartz raw materials and 1%-9% by mass of light-color conversion agent raw materials are weighed according to the total mass of raw material powder being 100%, and the raw materials are mixed evenly; 1%-3% of a silane coupling agent and the balance of raw material powder of a long afterglow material; s02, powder preparation: preparing a required long-afterglow material, namely SrAl2O4: Eu < 2 + >, Dy < 3 + > or Sr2MgSi2O7: Eu < 2 + >, Dy < 3 + >, by using a high-temperature solid-phase method, and sieving by using a sieve to obtain the required long-afterglow matrix material.The preparation method has the beneficial effect that the preparation of the color-adjustable light-storing ceramic is realized.
本发明适用于蓄光陶瓷领域,提供了一种颜色可调蓄光陶瓷及其制备方法,所述方法包括:S01:称量,以原料粉体总质量为100%计,分别称取质量百分比为35%~44%的10~30目的石英原料、35%~40%的50~100目的石英原料、5%~15%的150~250目的石英原料,1%~9%的光色转换剂原料,1%~3%的硅烷偶联剂,其余为长余辉材料的原料粉体;S02:制粉,利用高温固相法制备所需的长余辉材料,即SrAl2O4:Eu2+,Dy3+或Sr2MgSi2O7:Eu2+,Dy3+,并通过过筛网过筛,得到所需要的长余辉基质材料,本发明内容的有益效果在于:实现了颜色可调的蓄光陶瓷的制备。
Color-adjustable light storage ceramic and preparation method thereof
The invention is applicable to the field of light-storing ceramics, and provides a color-adjustable light-storing ceramic and a preparation method thereof.The method comprises the steps that S01, weighing is conducted, specifically, 35%-44% by mass of 10-30-mesh quartz raw materials, 35%-40% by mass of 50-100-mesh quartz raw materials, 5%-15% by mass of 150-250-mesh quartz raw materials and 1%-9% by mass of light-color conversion agent raw materials are weighed according to the total mass of raw material powder being 100%, and the raw materials are mixed evenly; 1%-3% of a silane coupling agent and the balance of raw material powder of a long afterglow material; s02, powder preparation: preparing a required long-afterglow material, namely SrAl2O4: Eu < 2 + >, Dy < 3 + > or Sr2MgSi2O7: Eu < 2 + >, Dy < 3 + >, by using a high-temperature solid-phase method, and sieving by using a sieve to obtain the required long-afterglow matrix material.The preparation method has the beneficial effect that the preparation of the color-adjustable light-storing ceramic is realized.
本发明适用于蓄光陶瓷领域,提供了一种颜色可调蓄光陶瓷及其制备方法,所述方法包括:S01:称量,以原料粉体总质量为100%计,分别称取质量百分比为35%~44%的10~30目的石英原料、35%~40%的50~100目的石英原料、5%~15%的150~250目的石英原料,1%~9%的光色转换剂原料,1%~3%的硅烷偶联剂,其余为长余辉材料的原料粉体;S02:制粉,利用高温固相法制备所需的长余辉材料,即SrAl2O4:Eu2+,Dy3+或Sr2MgSi2O7:Eu2+,Dy3+,并通过过筛网过筛,得到所需要的长余辉基质材料,本发明内容的有益效果在于:实现了颜色可调的蓄光陶瓷的制备。
Color-adjustable light storage ceramic and preparation method thereof
一种颜色可调蓄光陶瓷及其制备方法
ZHAO CHAO (author) / FENG YINGJUN (author) / CHEN YUE (author) / PENG JIANGLONG (author)
2023-01-03
Patent
Electronic Resource
Chinese
Fluorescent ceramic with adjustable light-emitting color and preparation method thereof
European Patent Office | 2020
|Zirconia ceramic with adjustable resistivity, porosity and color and preparation method thereof
European Patent Office | 2020
|Low-cost color-adjustable high-strength ceramic guide ring and preparation method thereof
European Patent Office | 2023
|Full-body color-changing light-transmitting ceramic tile and preparation method thereof
European Patent Office | 2020
|