A platform for research: civil engineering, architecture and urbanism
Anti-seepage construction method for basement bottom plate
The invention discloses an anti-seepage construction method for a basement bottom plate, which comprises the following steps of: pouring a C15 concrete cushion layer with the thickness of 100-150 on a basement foundation pit, then building a brick blank film in the pit between the foundation and a foundation surface, and pouring the C15 concrete cushion layer with the thickness of 100-150 on the foundation surface; according to the basement bottom plate anti-seepage construction method, the construction standard is standardized at the corners of the bottom plate structure and laying of waterproof materials, and the problems that in an existing basement bottom plate anti-seepage construction method, many corners of the bottom plate structure are not treated in place, and the construction cost is low are solved. The anti-seepage construction method for the basement bottom plate has the advantages that the corner treatment standard of the bottom plate structure is standardized, and meanwhile, the paving construction standard of the waterproof coiled materials is also defined, so that the situation that the subsequent bottom plate leaks due to the fact that the paving construction standard of the waterproof coiled materials is not clear is avoided.
本发明公开了一种地下室底板防渗漏施工方法,包括以下步骤:在地下室地基坑上浇筑100至150厚C15的混凝土垫层,然后在地基与地基面之间坑砌筑砖胎膜,在地基面浇筑100至150厚C15的混凝土垫层;随后在砖胎膜抹灰,在转角处做出50mm圆弧,涂刷基层处理剂,本发明通过对底板结构边角处和防水材料铺设进行规范施工标准,解决了目前的地下室底板防渗漏施工方法中存在很多底板结构边角细节处理不到位,及其防水卷材铺设施工标准不明确,从而造成后续底板出现渗漏的情况,该地下室底板防渗漏施工方法,具备规范了底板结构边角处理标准,同时还明确了防水卷材铺设施工标准的优点。
Anti-seepage construction method for basement bottom plate
The invention discloses an anti-seepage construction method for a basement bottom plate, which comprises the following steps of: pouring a C15 concrete cushion layer with the thickness of 100-150 on a basement foundation pit, then building a brick blank film in the pit between the foundation and a foundation surface, and pouring the C15 concrete cushion layer with the thickness of 100-150 on the foundation surface; according to the basement bottom plate anti-seepage construction method, the construction standard is standardized at the corners of the bottom plate structure and laying of waterproof materials, and the problems that in an existing basement bottom plate anti-seepage construction method, many corners of the bottom plate structure are not treated in place, and the construction cost is low are solved. The anti-seepage construction method for the basement bottom plate has the advantages that the corner treatment standard of the bottom plate structure is standardized, and meanwhile, the paving construction standard of the waterproof coiled materials is also defined, so that the situation that the subsequent bottom plate leaks due to the fact that the paving construction standard of the waterproof coiled materials is not clear is avoided.
本发明公开了一种地下室底板防渗漏施工方法,包括以下步骤:在地下室地基坑上浇筑100至150厚C15的混凝土垫层,然后在地基与地基面之间坑砌筑砖胎膜,在地基面浇筑100至150厚C15的混凝土垫层;随后在砖胎膜抹灰,在转角处做出50mm圆弧,涂刷基层处理剂,本发明通过对底板结构边角处和防水材料铺设进行规范施工标准,解决了目前的地下室底板防渗漏施工方法中存在很多底板结构边角细节处理不到位,及其防水卷材铺设施工标准不明确,从而造成后续底板出现渗漏的情况,该地下室底板防渗漏施工方法,具备规范了底板结构边角处理标准,同时还明确了防水卷材铺设施工标准的优点。
Anti-seepage construction method for basement bottom plate
一种地下室底板防渗漏施工方法
TAO XIAOQUAN (author) / ZHAN SHUXIONG (author) / CHEN MUXIONG (author) / CHEN SIBO (author) / LIN RUFEI (author) / CHEN HUIJUAN (author) / DENG XIN (author) / CHEN JUNSHEN (author) / LAI MINFENG (author) / YAO XIONGYE (author)
2023-01-31
Patent
Electronic Resource
Chinese
IPC:
E02D
FOUNDATIONS
,
Gründungen
Anti-seepage treatment method for basement bottom plate construction joint
European Patent Office | 2021
|Anti-seepage construction method for post-cast strip of basement bottom plate
European Patent Office | 2022
|Pressure type basement bottom plate anti-seepage drainage system
European Patent Office | 2023
|