The invention discloses a noctilucent decorative plate and a manufacturing method thereof. The noctilucent decorative plate structurally comprises a base plate, a pattern layer, a wear-resistant noctilucent layer and a scratch-resistant layer from bottom to top in sequence, the wear-resistant noctilucent layer is prepared from UV wear-resistant paint mixed with noctilucent powder according to the dosage of 70-150g/m < 2 >; the size of the noctilucent powder is 120 to 140 meshes; the mass ratio of the noctilucent powder to the UV wear-resistant coating is 1: 10; the manufacturing method of the noctilucent decorative plate comprises the steps that firstly, the pattern layer is manufactured on the base plate; then, the surface of the pattern layer is coated with UV wear-resistant paint mixed with noctilucent powder, and the dosage of the UV wear-resistant paint is 70-150 g/m < 2 >; then, a mercury lamp light source ultraviolet lamp is used for irradiation curing, and the light energy is adjusted to 240-280 mJ; the wear-resistant noctilucent layer is prepared; and finally, manufacturing a scratch-resistant layer on the surface of the wear-resistant noctilucent layer. According to the technical scheme, the light-emitting decorative plate has the light-emitting characteristic on the basis of ensuring the wear resistance.
一种夜光装饰板材及其制造方法,夜光装饰板材的结构为:自下而上依次为基板、图案层、耐磨夜光层和耐刮擦层;所述耐磨夜光层是由混有夜光粉的UV耐磨涂料按照70~150克/平方米用量制成;夜光粉的是120~140目;夜光粉和UV耐磨涂料的质量比例是1:10;所述夜光装饰板材的制作步骤包括:首先,先在基板上制作图案层;然后,将混有夜光粉的UV耐磨涂料涂到图案层表面,UV耐磨涂料的用量为70~150克/平方米;接着用汞灯光源紫外线灯进行照射固化,灯光能量调整到240~280mJ;制得耐磨夜光层;最后,在耐磨夜光层表面制作耐刮擦层。本技术方案在确保装饰板耐磨性能的基础上,具有发光特点。
The invention discloses a noctilucent decorative plate and a manufacturing method thereof. The noctilucent decorative plate structurally comprises a base plate, a pattern layer, a wear-resistant noctilucent layer and a scratch-resistant layer from bottom to top in sequence, the wear-resistant noctilucent layer is prepared from UV wear-resistant paint mixed with noctilucent powder according to the dosage of 70-150g/m < 2 >; the size of the noctilucent powder is 120 to 140 meshes; the mass ratio of the noctilucent powder to the UV wear-resistant coating is 1: 10; the manufacturing method of the noctilucent decorative plate comprises the steps that firstly, the pattern layer is manufactured on the base plate; then, the surface of the pattern layer is coated with UV wear-resistant paint mixed with noctilucent powder, and the dosage of the UV wear-resistant paint is 70-150 g/m < 2 >; then, a mercury lamp light source ultraviolet lamp is used for irradiation curing, and the light energy is adjusted to 240-280 mJ; the wear-resistant noctilucent layer is prepared; and finally, manufacturing a scratch-resistant layer on the surface of the wear-resistant noctilucent layer. According to the technical scheme, the light-emitting decorative plate has the light-emitting characteristic on the basis of ensuring the wear resistance.
一种夜光装饰板材及其制造方法,夜光装饰板材的结构为:自下而上依次为基板、图案层、耐磨夜光层和耐刮擦层;所述耐磨夜光层是由混有夜光粉的UV耐磨涂料按照70~150克/平方米用量制成;夜光粉的是120~140目;夜光粉和UV耐磨涂料的质量比例是1:10;所述夜光装饰板材的制作步骤包括:首先,先在基板上制作图案层;然后,将混有夜光粉的UV耐磨涂料涂到图案层表面,UV耐磨涂料的用量为70~150克/平方米;接着用汞灯光源紫外线灯进行照射固化,灯光能量调整到240~280mJ;制得耐磨夜光层;最后,在耐磨夜光层表面制作耐刮擦层。本技术方案在确保装饰板耐磨性能的基础上,具有发光特点。
Noctilucent decorative plate and manufacturing method thereof
一种夜光装饰板材及其制造方法
LI LIN (author)
2023-02-03
Patent
Electronic Resource
Chinese
IPC:
B05D
PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL
,
Verfahren zum Aufbringen von Flüssigkeiten oder von anderen fließfähigen Stoffen auf Oberflächen allgemein
/
E04F
FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS
,
Ausbau von Bauwerken, z.B. Treppen, Fußböden
Enamel noctilucent glaze, noctilucent enamel plate and manufacturing method
European Patent Office | 2022
|NOCTILUCENT FOOT PATH BLOCK AND MANUFACTURING METHOD THEREOF
European Patent Office | 2016
|DECORATIVE PLATE, METHOD OF MANUFACTURING DECORATIVE PLATE
European Patent Office | 2019
|