Building solid waste baking-free brick composite curing agent and baking-free brick prepared from same
According to the building solid waste baking-free brick composite curing agent and the baking-free brick prepared from the building solid waste baking-free brick composite curing agent, the baking-free brick is prepared from building waste fine powder particles, secondary pollution of the fine powder to the environment can be eliminated, the utilization rate of building waste can be increased, and a closed loop is formed. And the baking-free brick prepared from the baking-free brick has relatively high indexes of compressive strength, softening coefficient, freezing resistance and water resistance. According to the technical scheme, the curing agent is prepared from the following components in parts by weight: 10 parts of cement, 1 part of water glass, 2 parts of silica fume, 0.05 part of a composite water reducing agent and 1 part of wood fiber.
本发明提供了一种建筑固废免烧砖复合固化剂及其制成的免烧砖,其利用建筑垃圾细粉粒制备免烧砖,不仅能消除细粉料对环境的二次污染,还能提高建筑垃圾利用率并形成闭环。且用其制成免烧砖具有较高指标的抗压强度、软化系数、抗冻性和耐水性。其解决的技术方案是,该固化剂由以下成分按照重量比制成:水泥10份,水玻璃1份,微硅粉2份,复合减水剂0.05份,木质纤维1份。
Building solid waste baking-free brick composite curing agent and baking-free brick prepared from same
According to the building solid waste baking-free brick composite curing agent and the baking-free brick prepared from the building solid waste baking-free brick composite curing agent, the baking-free brick is prepared from building waste fine powder particles, secondary pollution of the fine powder to the environment can be eliminated, the utilization rate of building waste can be increased, and a closed loop is formed. And the baking-free brick prepared from the baking-free brick has relatively high indexes of compressive strength, softening coefficient, freezing resistance and water resistance. According to the technical scheme, the curing agent is prepared from the following components in parts by weight: 10 parts of cement, 1 part of water glass, 2 parts of silica fume, 0.05 part of a composite water reducing agent and 1 part of wood fiber.
本发明提供了一种建筑固废免烧砖复合固化剂及其制成的免烧砖,其利用建筑垃圾细粉粒制备免烧砖,不仅能消除细粉料对环境的二次污染,还能提高建筑垃圾利用率并形成闭环。且用其制成免烧砖具有较高指标的抗压强度、软化系数、抗冻性和耐水性。其解决的技术方案是,该固化剂由以下成分按照重量比制成:水泥10份,水玻璃1份,微硅粉2份,复合减水剂0.05份,木质纤维1份。
Building solid waste baking-free brick composite curing agent and baking-free brick prepared from same
一种建筑固废免烧砖复合固化剂及其制成的免烧砖
FAN LIUJUN (author) / TIAN GUOHUA (author) / LU XIAOMING (author) / LI MIN (author) / QIU LILI (author) / ZHU GUANG (author) / LIU HUANLING (author) / SUN CHUNJING (author) / YE BO (author)
2023-03-03
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Baking-free brick curing agent formula and baking-free brick preparation method
European Patent Office | 2021
|Formula of baking-free brick curing agent and baking-free brick preparation method
European Patent Office | 2021
|Calcium chloride baking-free brick curing agent and baking-free brick production process
European Patent Office | 2021
|Naphthalene water reducer baking-free brick curing agent and baking-free brick production process
European Patent Office | 2021
|European Patent Office | 2023
|