A platform for research: civil engineering, architecture and urbanism
Preparation method of anti-cracking lightweight interior wall plastering mortar
The invention provides a preparation method of anti-cracking light interior wall plastering mortar, and belongs to the technical field of buildings, and the anti-cracking light interior wall plastering mortar in the preparation method comprises the following main raw materials: 3-4 kg of gel powder, 35-45 kg of cement, 50-60 kg of quartz sand, 10-20 kg of light calcium carbonate, 10-20 kg of ash calcium powder and 20-40 kg of water. By readjusting the formula of the plastering mortar in the prior art, the strength and the adhesion of the existing plastering mortar can be enhanced, falling is avoided, the stability of the plastering mortar is guaranteed, cracking is avoided, the heat preservation effect is guaranteed, the smearing requirement is met, and the plastering mortar is applied and popularized in various technical fields of buildings; the adhesion and the anti-cracking effect are improved while the strength is ensured, so that the application is wider.
本发明提供一种防开裂轻质内墙抹灰砂浆制备方法,属于建筑技术领域,该防开裂轻质内墙抹灰砂浆制备方法中防开裂轻质内墙抹灰砂浆主要原料有:凝胶粉:3‑4kg,水泥:35‑45kg,石英砂:50‑60kg,轻质碳酸钙:10‑20kg,灰钙粉:10‑20kg,水20‑40kg。本发明通过对原有技术的抹灰砂浆配方重新调整,可增强现有抹灰砂浆的强度以及粘附性,并且避免脱落,保证其稳定性,避免开裂,并且保证保温效果,满足涂抹需求,应用推广与建筑各个技术领域中,抹灰砂浆的技术配方调整,保证了强度的同时还提高了粘附性以及防开裂效果,从而使得应用更加广泛。
Preparation method of anti-cracking lightweight interior wall plastering mortar
The invention provides a preparation method of anti-cracking light interior wall plastering mortar, and belongs to the technical field of buildings, and the anti-cracking light interior wall plastering mortar in the preparation method comprises the following main raw materials: 3-4 kg of gel powder, 35-45 kg of cement, 50-60 kg of quartz sand, 10-20 kg of light calcium carbonate, 10-20 kg of ash calcium powder and 20-40 kg of water. By readjusting the formula of the plastering mortar in the prior art, the strength and the adhesion of the existing plastering mortar can be enhanced, falling is avoided, the stability of the plastering mortar is guaranteed, cracking is avoided, the heat preservation effect is guaranteed, the smearing requirement is met, and the plastering mortar is applied and popularized in various technical fields of buildings; the adhesion and the anti-cracking effect are improved while the strength is ensured, so that the application is wider.
本发明提供一种防开裂轻质内墙抹灰砂浆制备方法,属于建筑技术领域,该防开裂轻质内墙抹灰砂浆制备方法中防开裂轻质内墙抹灰砂浆主要原料有:凝胶粉:3‑4kg,水泥:35‑45kg,石英砂:50‑60kg,轻质碳酸钙:10‑20kg,灰钙粉:10‑20kg,水20‑40kg。本发明通过对原有技术的抹灰砂浆配方重新调整,可增强现有抹灰砂浆的强度以及粘附性,并且避免脱落,保证其稳定性,避免开裂,并且保证保温效果,满足涂抹需求,应用推广与建筑各个技术领域中,抹灰砂浆的技术配方调整,保证了强度的同时还提高了粘附性以及防开裂效果,从而使得应用更加广泛。
Preparation method of anti-cracking lightweight interior wall plastering mortar
一种防开裂轻质内墙抹灰砂浆制备方法
GUO QIANGSHENG (author) / ZHOU JINFENG (author)
2023-03-14
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Preparation method of anti-cracking lightweight interior wall plastering gypsum
European Patent Office | 2023
|Anti-cracking and anti-cracking plastering mortar and preparation method thereof
European Patent Office | 2023
|Anti-cracking thin plastering mortar and preparation method thereof
European Patent Office | 2023
|