Composite high-temperature perovskite negative temperature coefficient thermistor and preparation method thereof
The invention discloses a composite high-temperature perovskite negative temperature coefficient thermistor and a preparation method thereof.The composite high-temperature perovskite negative temperature coefficient thermistor is prepared from calcium carbonate, zirconium dioxide and manganese dioxide according to the chemical formula (1-x) CaMn0. 05Zr0. 95O3-xCaMnO3, 0 < = x < = 0.2. The preparation method comprises the steps that a, perovskite phase CaMn0. 05Zr0. 95O3 is prepared; b, preparing a perovskite phase CaMnO3; and c, combining perovskite phases CaMn0. 05Zr0. 95 O3 and CaMnO3 to obtain the composite high-temperature perovskite negative temperature coefficient thermistor which has the negative temperature coefficient characteristic within the temperature range of 100-1200 DEG C and has the material constant of B100 DEG C/1200 DEG C = 1848.3-11286.4 K. The invention also discloses a preparation method of the composite high-temperature perovskite negative temperature coefficient thermistor. The composite high-temperature perovskite thermistor with the negative temperature coefficient is excellent in performance and good in high-temperature stability, and can provide support for temperature measurement in special environments such as high temperature.
本发明公开一种复合高温钙钛矿负温度系数热敏电阻及其制备方法,以碳酸钙、二氧化锆、二氧化锰为原料,按照化学式(1‑x)CaMn0.05Zr0.95O3‑xCaMnO3组成,其中0≤x≤0.2,其制备方法包括:a、制备钙钛矿相CaMn0.05Zr0.95O3;b、制备钙钛矿相CaMnO3;c、结合钙钛矿相CaMn0.05Zr0.95O3和CaMnO3得到在温度100℃‑1200℃范围内具有负温度系数特性,材料常数为B100℃/1200℃=1848.3‑11286.4K的复合高温钙钛矿负温度系数热敏电阻。该复合高温钙钛矿负温度系数热敏电阻性能优异,高温稳定性好,可以为高温等特殊环境的测温提供支持。
Composite high-temperature perovskite negative temperature coefficient thermistor and preparation method thereof
The invention discloses a composite high-temperature perovskite negative temperature coefficient thermistor and a preparation method thereof.The composite high-temperature perovskite negative temperature coefficient thermistor is prepared from calcium carbonate, zirconium dioxide and manganese dioxide according to the chemical formula (1-x) CaMn0. 05Zr0. 95O3-xCaMnO3, 0 < = x < = 0.2. The preparation method comprises the steps that a, perovskite phase CaMn0. 05Zr0. 95O3 is prepared; b, preparing a perovskite phase CaMnO3; and c, combining perovskite phases CaMn0. 05Zr0. 95 O3 and CaMnO3 to obtain the composite high-temperature perovskite negative temperature coefficient thermistor which has the negative temperature coefficient characteristic within the temperature range of 100-1200 DEG C and has the material constant of B100 DEG C/1200 DEG C = 1848.3-11286.4 K. The invention also discloses a preparation method of the composite high-temperature perovskite negative temperature coefficient thermistor. The composite high-temperature perovskite thermistor with the negative temperature coefficient is excellent in performance and good in high-temperature stability, and can provide support for temperature measurement in special environments such as high temperature.
本发明公开一种复合高温钙钛矿负温度系数热敏电阻及其制备方法,以碳酸钙、二氧化锆、二氧化锰为原料,按照化学式(1‑x)CaMn0.05Zr0.95O3‑xCaMnO3组成,其中0≤x≤0.2,其制备方法包括:a、制备钙钛矿相CaMn0.05Zr0.95O3;b、制备钙钛矿相CaMnO3;c、结合钙钛矿相CaMn0.05Zr0.95O3和CaMnO3得到在温度100℃‑1200℃范围内具有负温度系数特性,材料常数为B100℃/1200℃=1848.3‑11286.4K的复合高温钙钛矿负温度系数热敏电阻。该复合高温钙钛矿负温度系数热敏电阻性能优异,高温稳定性好,可以为高温等特殊环境的测温提供支持。
Composite high-temperature perovskite negative temperature coefficient thermistor and preparation method thereof
一种复合高温钙钛矿负温度系数热敏电阻及其制备方法
XIE YONGXIN (author) / WANG ZHENHUA (author) / LIU YUYU (author) / PAN YE (author) / ZHANG HUIMIN (author) / CHANG AIMIN (author)
2023-05-30
Patent
Electronic Resource
Chinese
High temperature negative temperature coefficient thermistor material and preparation method thereof
European Patent Office | 2020
|HIGH TEMPERATURE NEGATIVE TEMPERATURE COEFFICIENT THERMISTOR MATERIAL AND PREPARATION METHOD THEREOF
European Patent Office | 2019
|European Patent Office | 2024
|Preparation method of high-temperature negative temperature coefficient thermistor material
European Patent Office | 2020
|High-stability negative temperature coefficient thermistor material and preparation method thereof
European Patent Office | 2024
|