A platform for research: civil engineering, architecture and urbanism
Mortar material, preparation method and application thereof
The invention provides a mortar material as well as a preparation method and application thereof, and relates to the technical field of building materials. The mortar material is composed of the following components in percentage by mass: 15-25% of municipal waste incineration fly ash; 3%-15% of metakaolin; 3%-15% of fly ash; 1.3%-6.7% of silica fume; 28%-41.3% of water; 12.5%-16.5% of an alkali activator; 0.5%-2.5% of a thixotropic agent; 0.5%-20.8% of fine sand; and 1%-5% of fibers. The invention further provides application of the mortar material in the field of 3D building printing. The mortar material disclosed by the invention solves the problems that a printing material is relatively long in setting and hardening time, cannot meet the working performance of 3D building printing and is low in printing efficiency.
本发明提供了一种砂浆材料、制备方法及其应用,涉及建筑材料技术领域。按质量百分含量,所述砂浆材料由以下组分组成:城市垃圾焚烧飞灰15%‑25%;偏高岭土3%‑15%;粉煤灰3%‑15%;硅灰1.3%‑6.7%;水28%‑41.3%;碱激发剂12.5%‑16.5%;触变剂0.5%‑2.5%;细砂0.5%‑20.8%;纤维1%‑5%。本发明还提供了砂浆材料在3D建筑打印领域中的应用。本发明的砂浆材料解决了打印材料凝结硬化时间较长,无法满足3D建筑打印的工作性能以及打印效率低的问题。
Mortar material, preparation method and application thereof
The invention provides a mortar material as well as a preparation method and application thereof, and relates to the technical field of building materials. The mortar material is composed of the following components in percentage by mass: 15-25% of municipal waste incineration fly ash; 3%-15% of metakaolin; 3%-15% of fly ash; 1.3%-6.7% of silica fume; 28%-41.3% of water; 12.5%-16.5% of an alkali activator; 0.5%-2.5% of a thixotropic agent; 0.5%-20.8% of fine sand; and 1%-5% of fibers. The invention further provides application of the mortar material in the field of 3D building printing. The mortar material disclosed by the invention solves the problems that a printing material is relatively long in setting and hardening time, cannot meet the working performance of 3D building printing and is low in printing efficiency.
本发明提供了一种砂浆材料、制备方法及其应用,涉及建筑材料技术领域。按质量百分含量,所述砂浆材料由以下组分组成:城市垃圾焚烧飞灰15%‑25%;偏高岭土3%‑15%;粉煤灰3%‑15%;硅灰1.3%‑6.7%;水28%‑41.3%;碱激发剂12.5%‑16.5%;触变剂0.5%‑2.5%;细砂0.5%‑20.8%;纤维1%‑5%。本发明还提供了砂浆材料在3D建筑打印领域中的应用。本发明的砂浆材料解决了打印材料凝结硬化时间较长,无法满足3D建筑打印的工作性能以及打印效率低的问题。
Mortar material, preparation method and application thereof
一种砂浆材料、制备方法及其应用
WANG QING (author) / WANG XINRUI (author) / ZHANG QIANG (author) / DU YURONG (author) / MA XINYI (author) / CHEN GUANGYU (author)
2023-06-27
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
/
B33Y
ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
,
Additive (generative) Fertigung, d. h. die Herstellung von dreidimensionalen [3D] Bauteilen durch additive Abscheidung, additive Agglomeration oder additive Schichtung, z. B. durch 3D- Drucken, Stereolithografie oder selektives Lasersintern
Mortar material as well as preparation method and application thereof
European Patent Office | 2024
|Waterproof composite mortar material as well as preparation method and application thereof
European Patent Office | 2024
|Geopolymer mortar reinforcing material as well as preparation method and application thereof
European Patent Office | 2023
|Conductive mortar, preparation method thereof and auxiliary anode material
European Patent Office | 2023
|