The invention provides a liquid accelerator and a preparation method thereof, and relates to the technical field of accelerator preparation. The preparation method of the liquid accelerator comprises the following steps: 1) preparing a liquid sodium aluminate solution; 2) adding modified fluoride salt: adding water into the liquid sodium aluminate solution, and uniformly stirring; then adding the modified fluoride salt into the liquid sodium aluminate solution, stirring, and reacting for 0.5-1 hour at the temperature of 50-80 DEG C; 3) adding aluminum sulfate: adding aluminum sulfate within 10-30 minutes after the fluoride salt is completely reacted, and continuously reacting for 1-2 hours; and 4) adding organic alcohol amine, and stirring for 0.5-1 hour to obtain the liquid accelerator which has better viscosity stability.
本发明提供一种液体速凝剂及其制备方法,涉及速凝剂制备技术领域。液体速凝剂的制备方法,包括如下步骤:1)制备液体铝酸钠溶液;2)加入改性氟化盐:将水加入到所述液体铝酸钠溶液中,搅拌均匀;然后将所述改性氟化盐加入到所述液体铝酸钠溶液中,搅拌,50~80℃下反应0.5~1h;3)加入硫酸铝:在氟化盐反应完全后的10~30min内,添加硫酸铝,继续反应1~2h;4)加入有机醇胺,搅拌0.5~1h即制得液体速凝剂,该液体速凝剂具有较好的粘度稳定性。
Liquid accelerator and preparation method thereof
The invention provides a liquid accelerator and a preparation method thereof, and relates to the technical field of accelerator preparation. The preparation method of the liquid accelerator comprises the following steps: 1) preparing a liquid sodium aluminate solution; 2) adding modified fluoride salt: adding water into the liquid sodium aluminate solution, and uniformly stirring; then adding the modified fluoride salt into the liquid sodium aluminate solution, stirring, and reacting for 0.5-1 hour at the temperature of 50-80 DEG C; 3) adding aluminum sulfate: adding aluminum sulfate within 10-30 minutes after the fluoride salt is completely reacted, and continuously reacting for 1-2 hours; and 4) adding organic alcohol amine, and stirring for 0.5-1 hour to obtain the liquid accelerator which has better viscosity stability.
本发明提供一种液体速凝剂及其制备方法,涉及速凝剂制备技术领域。液体速凝剂的制备方法,包括如下步骤:1)制备液体铝酸钠溶液;2)加入改性氟化盐:将水加入到所述液体铝酸钠溶液中,搅拌均匀;然后将所述改性氟化盐加入到所述液体铝酸钠溶液中,搅拌,50~80℃下反应0.5~1h;3)加入硫酸铝:在氟化盐反应完全后的10~30min内,添加硫酸铝,继续反应1~2h;4)加入有机醇胺,搅拌0.5~1h即制得液体速凝剂,该液体速凝剂具有较好的粘度稳定性。
Liquid accelerator and preparation method thereof
一种液体速凝剂及其制备方法
FAN DONGDONG (author) / ZHU ZONGJIAN (author) / LIN CHUNHONG (author) / YU CHUNSONG (author) / WANG ZHIYONG (author) / CHEN JIN (author) / HUANG HAI (author) / JIANG AJUAN (author) / YU JINNAN (author)
2023-10-13
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Alkaline liquid accelerator and preparation method thereof
European Patent Office | 2021
|