A platform for research: civil engineering, architecture and urbanism
Decorative mortar for forming litchi surface, decorative slurry, preparation method and forming method
The invention provides decorative mortar and decorative slurry for forming a litchi surface, and a preparation and formation method of the decorative mortar and the decorative slurry. The decorative mortar is prepared from the following components in parts by mass: 18 to 22 parts of white cement, 9 to 11 parts of heavy calcium carbonate, 16 to 20 parts of first quartz sand, 13 to 15 parts of second quartz sand, 11 to 13 parts of third quartz sand, 21 to 25 parts of calcium sand, 1.5 to 2.5 parts of rubber powder, 0.18 to 0.22 part of water-retaining agent, 0.28 to 0.32 part of lignocellulose and 0.0019 to 0.0021 part of air entraining agent. According to the decorative mortar for forming the litchi surface, through reasonable arrangement of the components and the proportion, on one hand, the quartz sand and the calcium sand form continuous grading, forming of uniformly-distributed and uneven textures of a decorative surface is facilitated, and on the other hand, the decorative slurry formed by the decorative mortar meets the conditions of spraying construction; therefore, the influence of construction methods of constructors on the formed litchi surface is reduced.
本发明提供了一种用于形成荔枝面的装饰砂浆、装饰浆料、制备及形成方法。该装饰砂浆以质量份计包括:白水泥18~22份、重钙9~11份、第一石英砂16~20份、第二石英砂13~15份、第三石英砂11~13份、钙砂21~25份、胶粉1.5~2.5份、保水剂0.18~0.22份、木质纤维素0.28~0.32份和引气剂0.0019~0.0021份。上述的用于形成荔枝面的装饰砂浆,通过合理设置各组分及配比,一方面使得石英砂和钙砂形成连续级配,有助于形成饰面呈现均匀分布的、凹凸不平的纹理,另一方面使得装饰砂浆形成的装饰浆料满足喷涂施工的条件,从而减少施工人员的施工手法对形成荔枝面的影响。
Decorative mortar for forming litchi surface, decorative slurry, preparation method and forming method
The invention provides decorative mortar and decorative slurry for forming a litchi surface, and a preparation and formation method of the decorative mortar and the decorative slurry. The decorative mortar is prepared from the following components in parts by mass: 18 to 22 parts of white cement, 9 to 11 parts of heavy calcium carbonate, 16 to 20 parts of first quartz sand, 13 to 15 parts of second quartz sand, 11 to 13 parts of third quartz sand, 21 to 25 parts of calcium sand, 1.5 to 2.5 parts of rubber powder, 0.18 to 0.22 part of water-retaining agent, 0.28 to 0.32 part of lignocellulose and 0.0019 to 0.0021 part of air entraining agent. According to the decorative mortar for forming the litchi surface, through reasonable arrangement of the components and the proportion, on one hand, the quartz sand and the calcium sand form continuous grading, forming of uniformly-distributed and uneven textures of a decorative surface is facilitated, and on the other hand, the decorative slurry formed by the decorative mortar meets the conditions of spraying construction; therefore, the influence of construction methods of constructors on the formed litchi surface is reduced.
本发明提供了一种用于形成荔枝面的装饰砂浆、装饰浆料、制备及形成方法。该装饰砂浆以质量份计包括:白水泥18~22份、重钙9~11份、第一石英砂16~20份、第二石英砂13~15份、第三石英砂11~13份、钙砂21~25份、胶粉1.5~2.5份、保水剂0.18~0.22份、木质纤维素0.28~0.32份和引气剂0.0019~0.0021份。上述的用于形成荔枝面的装饰砂浆,通过合理设置各组分及配比,一方面使得石英砂和钙砂形成连续级配,有助于形成饰面呈现均匀分布的、凹凸不平的纹理,另一方面使得装饰砂浆形成的装饰浆料满足喷涂施工的条件,从而减少施工人员的施工手法对形成荔枝面的影响。
Decorative mortar for forming litchi surface, decorative slurry, preparation method and forming method
用于形成荔枝面的装饰砂浆、装饰浆料、制备及形成方法
DAI JIAN (author) / CHEN CHANGMING (author) / WU YUHONG (author) / SU FENG (author)
2023-10-20
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2023
|Decorative mortar as well as preparation method and construction method of decorative mortar
European Patent Office | 2024
|Decorative Concrete - Forming for Decorative Concrete
Online Contents | 2005