Brick red tea spar ceramic and preparation method thereof
The invention belongs to the technical field of ceramic preparation, and discloses brick red tea spar ceramic and a preparation method thereof. The preparation method comprises the following steps: mixing and ball-milling tea spar, Fe2O3 and a grinding medium to obtain slurry; drying, grinding and sieving the slurry, and performing compression molding to obtain a blank; and sintering the green body to obtain the brick red tea spar ceramic. The brick-red tea spar ceramic prepared by using a high-temperature solid-phase method has the advantages of stable color generation, uniform color distribution, hardness of 5.5-8.5 GPa, good mechanical properties, cheap Fe2O3 coloring agent, green and pollution-free preparation method, low energy consumption and high production efficiency, increases the types of ceramics using tea spar as the raw material, and has a wide application prospect. And the market competitiveness of the red ceramic product is improved.
本发明属于陶瓷制备技术领域,公开了一种砖红色茶晶石陶瓷及其制备方法。本发明所述制备方法包括步骤:将茶晶石、Fe2O3和研磨介质混合球磨,得到浆料;浆料干燥、研磨过筛、压制成型,得到胚体;胚体烧结,得到砖红色茶晶石陶瓷。本发明利用高温固相法制备出砖红色茶晶石陶瓷,呈色稳定,亮度值为40~80cd/m2,色彩分布均匀,硬度可达到5.5~8.5GPa,力学性能较好,Fe2O3着色剂价格便宜,制备方法绿色无污染,能耗低,生产效率高,且增加了以茶晶石为原料的陶瓷种类,提升了红色陶瓷制品的市场竞争力。
Brick red tea spar ceramic and preparation method thereof
The invention belongs to the technical field of ceramic preparation, and discloses brick red tea spar ceramic and a preparation method thereof. The preparation method comprises the following steps: mixing and ball-milling tea spar, Fe2O3 and a grinding medium to obtain slurry; drying, grinding and sieving the slurry, and performing compression molding to obtain a blank; and sintering the green body to obtain the brick red tea spar ceramic. The brick-red tea spar ceramic prepared by using a high-temperature solid-phase method has the advantages of stable color generation, uniform color distribution, hardness of 5.5-8.5 GPa, good mechanical properties, cheap Fe2O3 coloring agent, green and pollution-free preparation method, low energy consumption and high production efficiency, increases the types of ceramics using tea spar as the raw material, and has a wide application prospect. And the market competitiveness of the red ceramic product is improved.
本发明属于陶瓷制备技术领域,公开了一种砖红色茶晶石陶瓷及其制备方法。本发明所述制备方法包括步骤:将茶晶石、Fe2O3和研磨介质混合球磨,得到浆料;浆料干燥、研磨过筛、压制成型,得到胚体;胚体烧结,得到砖红色茶晶石陶瓷。本发明利用高温固相法制备出砖红色茶晶石陶瓷,呈色稳定,亮度值为40~80cd/m2,色彩分布均匀,硬度可达到5.5~8.5GPa,力学性能较好,Fe2O3着色剂价格便宜,制备方法绿色无污染,能耗低,生产效率高,且增加了以茶晶石为原料的陶瓷种类,提升了红色陶瓷制品的市场竞争力。
Brick red tea spar ceramic and preparation method thereof
一种砖红色茶晶石陶瓷及其制备方法
BAO JINXIAO (author) / BIAN ZHENHU (author) / WANG QINGCHUN (author) / RUAN FEI (author) / HAI WENZHI (author) / MA YUWEI (author) / SHANG WEIXIANG (author) / LI HONGXIA (author)
2023-10-27
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Electrothermal composite ceramic brick and preparation method thereof
European Patent Office | 2015
|Building ceramic plate/brick and preparation method thereof
European Patent Office | 2021
|Glass-ceramic composite brick and preparation method thereof
European Patent Office | 2021
|