A platform for research: civil engineering, architecture and urbanism
Microwave dielectric ceramic with low dielectric constant and low loss and preparation method thereof
The invention discloses a microwave dielectric ceramic with low dielectric constant and low loss and a preparation method thereof, the chemical composition expression of the microwave dielectric ceramic is CaLaAl3O7, and the microwave dielectric ceramic has low dielectric constant (5.8-6.3), low loss (7.2 * 10 <-4 >) and negative temperature coefficient of resonance frequency (-37 to-31 ppm/DEG C). The microwave dielectric ceramic has low dielectric constant and lower loss, is an ideal candidate material of low-dielectric microwave ceramics in the field of wireless communication, is prepared by adopting a traditional solid-phase reaction method, is mature in process, can be industrially produced, is high in reproducibility and can be used for synthesizing a stable pure phase.
本发明公开了一种低介电常数低损耗的微波介质陶瓷及其制备方法,本发明的微波介质陶瓷的化学组成表达式为CaLaAl3O7,其具有低介电常数(5.8~6.3),低损耗(7.2×10‑4)以及负的谐振频率温度系数(‑37~‑31ppm/℃)。本发明的微波介质陶瓷具有低介电常数与较低损耗,是无线通信领域低介电微波陶瓷的理想候选材料,同时采用传统固相反应法制备,工艺成熟且可工业化生产,复现性强且能合成稳定的纯相。
Microwave dielectric ceramic with low dielectric constant and low loss and preparation method thereof
The invention discloses a microwave dielectric ceramic with low dielectric constant and low loss and a preparation method thereof, the chemical composition expression of the microwave dielectric ceramic is CaLaAl3O7, and the microwave dielectric ceramic has low dielectric constant (5.8-6.3), low loss (7.2 * 10 <-4 >) and negative temperature coefficient of resonance frequency (-37 to-31 ppm/DEG C). The microwave dielectric ceramic has low dielectric constant and lower loss, is an ideal candidate material of low-dielectric microwave ceramics in the field of wireless communication, is prepared by adopting a traditional solid-phase reaction method, is mature in process, can be industrially produced, is high in reproducibility and can be used for synthesizing a stable pure phase.
本发明公开了一种低介电常数低损耗的微波介质陶瓷及其制备方法,本发明的微波介质陶瓷的化学组成表达式为CaLaAl3O7,其具有低介电常数(5.8~6.3),低损耗(7.2×10‑4)以及负的谐振频率温度系数(‑37~‑31ppm/℃)。本发明的微波介质陶瓷具有低介电常数与较低损耗,是无线通信领域低介电微波陶瓷的理想候选材料,同时采用传统固相反应法制备,工艺成熟且可工业化生产,复现性强且能合成稳定的纯相。
Microwave dielectric ceramic with low dielectric constant and low loss and preparation method thereof
一种低介电常数低损耗的微波介质陶瓷及其制备方法
LI ENZHU (author) / ZHENG YIXUAN (author) / HU ZHICHAO (author) / ZHONG CHAOWEI (author) / ZHANG SHUREN (author)
2024-01-16
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2021
|European Patent Office | 2015
|Low-dielectric-constant microwave dielectric ceramic and preparation method thereof
European Patent Office | 2020
|Medium dielectric constant microwave dielectric ceramic and preparation method thereof
European Patent Office | 2024
|European Patent Office | 2021
|