A platform for research: civil engineering, architecture and urbanism
Environment-friendly cement-based polymer waterproof mortar and preparation method thereof
The invention relates to environment-friendly cement-based polymer waterproof mortar. The building material is prepared from the following components in parts by weight: 15-25 parts of Portland cement, 3-6 parts of carborundum powder, 4-8 parts of serpentine, 15-25 parts of fly ash, 3-5 parts of sepiolite fiber, 1-3 parts of regenerated glass fiber reinforced plastic fiber, 2-4 parts of water-soluble polyphenylene sulfide, 1-4 parts of sulfonate type hyperbranched polyurethane emulsion, 1-3 parts of beta-nicotinamide adenine dinucleotide modified 1, 3, 4-trimethyl-1, 3-pentanediol monoisobutyrate, 1-3 parts of sodium dodecyl benzene sulfonate, 1-3 parts of sodium dodecyl benzene sulfonate and 1-3 parts of sodium dodecyl benzene sulfonate. And 0.3 to 0.6 part of 1, 3, 5-triglycidyl-S-triazinetrione, and 10 to 20 parts of water. The invention also discloses a preparation method of the environment-friendly cement-based polymer waterproof mortar. The environment-friendly cement-based polymer waterproof mortar disclosed by the invention is good in impermeability and waterproofness, high in strength, sufficient in durability and toughness, excellent in water absorption, toughness and breaking strength, high in bonding strength with a base material, and safe and environment-friendly to use.
一种环保水泥基聚合物防水砂浆,其特征在于,是由如下按重量份计的各组分制成:硅酸盐水泥15‑25份、金刚砂粉3‑6份、蛇纹石4‑8份、粉煤灰15‑25份、海泡石纤维3‑5份、再生玻璃钢纤维1‑3份、水溶性聚苯硫醚2‑4份、磺酸盐型超支化聚氨酯乳液1‑4份、β‑烟酰胺腺嘌呤二核苷酸改性1,3,5‑三缩水甘油‑S‑三嗪三酮0.3‑0.6份、水10‑20份。本发明还公开了所述环保水泥基聚合物防水砂浆的制备方法。本发明公开的环保水泥基聚合物防水砂浆抗渗性、防水性佳,强度大,耐用性、韧性足,吸水率、韧性以及抗折强度优异,与基材的粘结强度大,使用安全环保。
Environment-friendly cement-based polymer waterproof mortar and preparation method thereof
The invention relates to environment-friendly cement-based polymer waterproof mortar. The building material is prepared from the following components in parts by weight: 15-25 parts of Portland cement, 3-6 parts of carborundum powder, 4-8 parts of serpentine, 15-25 parts of fly ash, 3-5 parts of sepiolite fiber, 1-3 parts of regenerated glass fiber reinforced plastic fiber, 2-4 parts of water-soluble polyphenylene sulfide, 1-4 parts of sulfonate type hyperbranched polyurethane emulsion, 1-3 parts of beta-nicotinamide adenine dinucleotide modified 1, 3, 4-trimethyl-1, 3-pentanediol monoisobutyrate, 1-3 parts of sodium dodecyl benzene sulfonate, 1-3 parts of sodium dodecyl benzene sulfonate and 1-3 parts of sodium dodecyl benzene sulfonate. And 0.3 to 0.6 part of 1, 3, 5-triglycidyl-S-triazinetrione, and 10 to 20 parts of water. The invention also discloses a preparation method of the environment-friendly cement-based polymer waterproof mortar. The environment-friendly cement-based polymer waterproof mortar disclosed by the invention is good in impermeability and waterproofness, high in strength, sufficient in durability and toughness, excellent in water absorption, toughness and breaking strength, high in bonding strength with a base material, and safe and environment-friendly to use.
一种环保水泥基聚合物防水砂浆,其特征在于,是由如下按重量份计的各组分制成:硅酸盐水泥15‑25份、金刚砂粉3‑6份、蛇纹石4‑8份、粉煤灰15‑25份、海泡石纤维3‑5份、再生玻璃钢纤维1‑3份、水溶性聚苯硫醚2‑4份、磺酸盐型超支化聚氨酯乳液1‑4份、β‑烟酰胺腺嘌呤二核苷酸改性1,3,5‑三缩水甘油‑S‑三嗪三酮0.3‑0.6份、水10‑20份。本发明还公开了所述环保水泥基聚合物防水砂浆的制备方法。本发明公开的环保水泥基聚合物防水砂浆抗渗性、防水性佳,强度大,耐用性、韧性足,吸水率、韧性以及抗折强度优异,与基材的粘结强度大,使用安全环保。
Environment-friendly cement-based polymer waterproof mortar and preparation method thereof
一种环保水泥基聚合物防水砂浆及其制备方法
LIU CHUNPING (author) / YUAN QUAN (author) / YANG CHEN (author) / TANG CUILI (author) / XUN XIANGYU (author)
2024-02-09
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Cement-based polymer waterproof mortar and preparation method thereof
European Patent Office | 2024
|Waterproof and permeable cement-based polymer waterproof mortar and preparation method thereof
European Patent Office | 2020
|Environment-friendly polymer waterproof thermal insulation mortar
European Patent Office | 2020
|Waterproof heat insulation environment-friendly mortar and preparation method thereof
European Patent Office | 2015
|Waterproof anti-crack environment-friendly mortar and preparation method thereof
European Patent Office | 2021
|