A platform for research: civil engineering, architecture and urbanism
Waterproof crystallization anti-seepage and anti-crack material applied to basement
The invention relates to the technical field of building materials, and discloses a waterproof crystallization anti-seepage anti-crack material applied to basements, which is prepared by the following preparation steps: step 1, preparing a class A water absorption composition; 2, stirring and mixing the prepared A-type water absorption composition and Portland cement, and sequentially adding a crystallization control agent and a waterproof agent into the obtained mixture; step 3, continuing to add a waterproof agent into the mixture obtained in the step 2 to obtain an anti-permeability composition; 4, one or more of silicon oxide, aluminum oxide, crystalline titanium dioxide and calcium carbonate are mixed or taken independently, and superfine active crystal powder is obtained; 5, stirring and mixing the polymer emulsion, the flexibilizer, the hydrated calcium silicate, the nanoparticles and the superfine active crystal powder to obtain an anti-cracking composition; and step 6, stirring the anti-seepage composition, the anti-crack composition and the adhesive together, and increasing the temperature in the container to enhance the molecular activeness of the anti-seepage composition, the anti-crack composition and the adhesive, thereby finally obtaining the anti-seepage and anti-crack material.
本发明涉及建筑材料技术领域,且公开了一种应用于地下室的防水结晶抗渗抗裂材料,包括以下制备步骤:步骤一、制备A类吸水组合物;步骤二、将制备所得的A类吸水组合物与硅酸盐水泥进行搅拌混合,得到的混合物依次向其中加入结晶控制剂和防水剂;步骤三、继续向步骤二所得的混合物内加入防水剂,得到抗渗组合物;步骤四、将氧化硅、氧化铝、晶态二氧化钛和碳酸钙其中一种或多种进行混合或单独取用,得到超细活性结晶粉;步骤五、将聚合物乳液、增韧剂、水化硅酸钙和纳米颗粒与超细活性结晶粉搅拌混合得到抗裂组合物;步骤六、将抗渗组合物、抗裂组合物和粘合剂共同搅拌,同时容器内温度升温增强三者分子活跃度,最后得到抗渗抗裂材料。
Waterproof crystallization anti-seepage and anti-crack material applied to basement
The invention relates to the technical field of building materials, and discloses a waterproof crystallization anti-seepage anti-crack material applied to basements, which is prepared by the following preparation steps: step 1, preparing a class A water absorption composition; 2, stirring and mixing the prepared A-type water absorption composition and Portland cement, and sequentially adding a crystallization control agent and a waterproof agent into the obtained mixture; step 3, continuing to add a waterproof agent into the mixture obtained in the step 2 to obtain an anti-permeability composition; 4, one or more of silicon oxide, aluminum oxide, crystalline titanium dioxide and calcium carbonate are mixed or taken independently, and superfine active crystal powder is obtained; 5, stirring and mixing the polymer emulsion, the flexibilizer, the hydrated calcium silicate, the nanoparticles and the superfine active crystal powder to obtain an anti-cracking composition; and step 6, stirring the anti-seepage composition, the anti-crack composition and the adhesive together, and increasing the temperature in the container to enhance the molecular activeness of the anti-seepage composition, the anti-crack composition and the adhesive, thereby finally obtaining the anti-seepage and anti-crack material.
本发明涉及建筑材料技术领域,且公开了一种应用于地下室的防水结晶抗渗抗裂材料,包括以下制备步骤:步骤一、制备A类吸水组合物;步骤二、将制备所得的A类吸水组合物与硅酸盐水泥进行搅拌混合,得到的混合物依次向其中加入结晶控制剂和防水剂;步骤三、继续向步骤二所得的混合物内加入防水剂,得到抗渗组合物;步骤四、将氧化硅、氧化铝、晶态二氧化钛和碳酸钙其中一种或多种进行混合或单独取用,得到超细活性结晶粉;步骤五、将聚合物乳液、增韧剂、水化硅酸钙和纳米颗粒与超细活性结晶粉搅拌混合得到抗裂组合物;步骤六、将抗渗组合物、抗裂组合物和粘合剂共同搅拌,同时容器内温度升温增强三者分子活跃度,最后得到抗渗抗裂材料。
Waterproof crystallization anti-seepage and anti-crack material applied to basement
一种应用于地下室的防水结晶抗渗抗裂材料
2024-03-12
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Waterproof and anti-seepage basement structure and construction method thereof
European Patent Office | 2024
|Anti-crack and anti-seepage construction equipment for basement with concrete structure
European Patent Office | 2023
|Preparation method of nano-modified anti-seepage anti-crack waterproof agent
European Patent Office | 2022
|Basement anti-seepage flame-retardant sound insulation material
European Patent Office | 2023
|