Imitation ceramic handicraft and preparation method thereof
The invention discloses an imitation ceramic handicraft and a preparation method thereof. The imitation ceramic handicraft comprises the following components in parts by weight: 30-35 parts of ceramic powder, 15-20 parts of quartz sand powder, 5-8 parts of epoxy resin, 3-5 parts of glass fiber, 5-8 parts of magnesium chloride, 3-5 parts of magnesium oxide, 2-3 parts of calcium oxide, 3-5 parts of phenolsulfonic acid, 2-3 parts of lauryl sodium sulfate, 2-3 parts of polyvinyl acetate and 5-8 parts of polyacrylamide. By controlling and mixing the components in parts by weight, the slurry has good flowing property and forming property, and the slurry and the remaining components are polymerized by the phenolsulfonic acid, the lauryl sodium sulfate, the polyvinyl acetate, the polyacrylamide and other components to form a compact structure, so that cracks formed by the mixed slurry can be reduced; after the components are compounded, the mold-opened handicraft has a heavy feeling similar to that of ceramic, crack damage is reduced, a better molding shape is achieved, and the manufactured handicraft is good in later mechanical performance, good in strength and impact resistance and more wear-resistant.
本发明公开了一种仿陶瓷工艺品及其制备方法,仿陶瓷工艺品包括以下重量份数的组分:陶瓷粉30~35份、石英砂粉15~20份、环氧树脂5~8份、玻璃纤维3~5份、氯化镁5~8份、氧化镁3~5份、氧化钙2~3份、苯酚磺酸3~5份、十二烷基硫酸钠2~3份、聚醋酸乙烯酯2~3份、聚丙烯酰胺5~8份。通过控制各组分之间的重量份比混合,使浆料具有良好的流动性能和成型性能,而苯酚磺酸、十二烷基硫酸钠、聚醋酸乙烯酯、聚丙烯酰胺等组分将浆料和剩余组分聚合起来,形成紧密的结构,能减小混合浆料形成的裂纹,各组分复配后使开模后的工艺品形成类似陶瓷的质重感,减少了裂缝破损,更好的塑造形状,制成的工艺品的后期机械性能良好,具有良好的强度、抗冲击性和更耐磨。
Imitation ceramic handicraft and preparation method thereof
The invention discloses an imitation ceramic handicraft and a preparation method thereof. The imitation ceramic handicraft comprises the following components in parts by weight: 30-35 parts of ceramic powder, 15-20 parts of quartz sand powder, 5-8 parts of epoxy resin, 3-5 parts of glass fiber, 5-8 parts of magnesium chloride, 3-5 parts of magnesium oxide, 2-3 parts of calcium oxide, 3-5 parts of phenolsulfonic acid, 2-3 parts of lauryl sodium sulfate, 2-3 parts of polyvinyl acetate and 5-8 parts of polyacrylamide. By controlling and mixing the components in parts by weight, the slurry has good flowing property and forming property, and the slurry and the remaining components are polymerized by the phenolsulfonic acid, the lauryl sodium sulfate, the polyvinyl acetate, the polyacrylamide and other components to form a compact structure, so that cracks formed by the mixed slurry can be reduced; after the components are compounded, the mold-opened handicraft has a heavy feeling similar to that of ceramic, crack damage is reduced, a better molding shape is achieved, and the manufactured handicraft is good in later mechanical performance, good in strength and impact resistance and more wear-resistant.
本发明公开了一种仿陶瓷工艺品及其制备方法,仿陶瓷工艺品包括以下重量份数的组分:陶瓷粉30~35份、石英砂粉15~20份、环氧树脂5~8份、玻璃纤维3~5份、氯化镁5~8份、氧化镁3~5份、氧化钙2~3份、苯酚磺酸3~5份、十二烷基硫酸钠2~3份、聚醋酸乙烯酯2~3份、聚丙烯酰胺5~8份。通过控制各组分之间的重量份比混合,使浆料具有良好的流动性能和成型性能,而苯酚磺酸、十二烷基硫酸钠、聚醋酸乙烯酯、聚丙烯酰胺等组分将浆料和剩余组分聚合起来,形成紧密的结构,能减小混合浆料形成的裂纹,各组分复配后使开模后的工艺品形成类似陶瓷的质重感,减少了裂缝破损,更好的塑造形状,制成的工艺品的后期机械性能良好,具有良好的强度、抗冲击性和更耐磨。
Imitation ceramic handicraft and preparation method thereof
一种仿陶瓷工艺品及其制备方法
XU WEI (author) / JIANG YANHUA (author) / NIE YALI (author)
2024-04-30
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Antibacterial and mildew-proof ceramic handicraft and preparation method thereof
European Patent Office | 2023
|European Patent Office | 2024
|European Patent Office | 2024
|