The invention discloses a self-leveling master batch for a corundum terrace. The self-leveling master batch comprises the following components in parts by weight: 300-400 parts of anti-cracking double-fast high belite sulphoaluminate cement; 10 to 30 parts of nano silicon powder; 300 to 600 parts of diamond; 50 to 100 parts of glass sand powder; 10 to 100 parts of microbead powder; 15 to 30 parts of rubber powder; 1-5 parts of a flowable agent; 0.5 to 1 part of an anti-settling water-retaining agent; 0.5-2 parts of a foam guiding agent; 3-10 parts of an accelerator; 0.5-2 parts of a time drying agent; 120 to 130 parts of water; compared with the prior art, the nano silicon powder, the glass sand powder and the microbead powder serve as filling materials, the diamond serves as aggregate, the nano silicon powder increases compactness and increases early strength, the glass sand powder plays a role in polishing and grinding brightness, the microbead powder increases self-leveling high flow state, and the diamond increases core abrasion resistance strength; all the components are matched, so that the shrinkage-expansion rate of the emery terrace self-leveling master batch can be controlled to be about three ten thousandths.
本发明公开了一种金钢砂地坪自流平母料,按照重量份数计算包括以下各组分:抗裂双快高贝利特硫铝酸盐水泥300‑400份;纳米硅粉10‑30份;金刚石300‑600份;玻璃砂粉50‑100份;微珠粉10‑100份;胶粉15‑30份;流动剂1‑5份;防沉降保水剂0.5‑1份;引泡剂0.5‑2份;速凝剂3‑10份;时间干燥剂0.5‑2份;水120‑130份;本发明与现有技术相比,由纳米硅粉、玻璃砂粉以及微珠粉作为填充料,金刚石作为骨料,纳米硅粉增加密实度及增加早期强度,玻璃砂粉起抛光研磨亮度,微珠粉增加自流平高流态,金刚石增加核心耐磨度强度,且各组分配合来使金钢砂地坪自流平母料能够将收缩膨胀率控制在万分之三左右。
The invention discloses a self-leveling master batch for a corundum terrace. The self-leveling master batch comprises the following components in parts by weight: 300-400 parts of anti-cracking double-fast high belite sulphoaluminate cement; 10 to 30 parts of nano silicon powder; 300 to 600 parts of diamond; 50 to 100 parts of glass sand powder; 10 to 100 parts of microbead powder; 15 to 30 parts of rubber powder; 1-5 parts of a flowable agent; 0.5 to 1 part of an anti-settling water-retaining agent; 0.5-2 parts of a foam guiding agent; 3-10 parts of an accelerator; 0.5-2 parts of a time drying agent; 120 to 130 parts of water; compared with the prior art, the nano silicon powder, the glass sand powder and the microbead powder serve as filling materials, the diamond serves as aggregate, the nano silicon powder increases compactness and increases early strength, the glass sand powder plays a role in polishing and grinding brightness, the microbead powder increases self-leveling high flow state, and the diamond increases core abrasion resistance strength; all the components are matched, so that the shrinkage-expansion rate of the emery terrace self-leveling master batch can be controlled to be about three ten thousandths.
本发明公开了一种金钢砂地坪自流平母料,按照重量份数计算包括以下各组分:抗裂双快高贝利特硫铝酸盐水泥300‑400份;纳米硅粉10‑30份;金刚石300‑600份;玻璃砂粉50‑100份;微珠粉10‑100份;胶粉15‑30份;流动剂1‑5份;防沉降保水剂0.5‑1份;引泡剂0.5‑2份;速凝剂3‑10份;时间干燥剂0.5‑2份;水120‑130份;本发明与现有技术相比,由纳米硅粉、玻璃砂粉以及微珠粉作为填充料,金刚石作为骨料,纳米硅粉增加密实度及增加早期强度,玻璃砂粉起抛光研磨亮度,微珠粉增加自流平高流态,金刚石增加核心耐磨度强度,且各组分配合来使金钢砂地坪自流平母料能够将收缩膨胀率控制在万分之三左右。
Self-leveling master batch for emery terrace and preparation method of self-leveling master batch
一种金钢砂地坪自流平母料及其制备方法
LUO AO (author)
2024-05-03
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Production formula and production method of gypsum self-leveling master batch