Preparation method of high-adhesion two-component interface leveling material for tile renovation
The invention discloses a preparation method of a high-adhesion two-component interface leveling material for tile renovation. The raw materials comprise 10-30 parts of deionized water; 0.1 to 1 part of cellulose; 0.1 to 1 part of bentonite; 0.1-1 part of a dispersant; 0.1 to 1 part of a defoaming agent; 0.1-1 part of a preservative; 0.1-2 parts of a coalescing agent; 0.1 to 1 part of a pH regulator; 0.1-2 parts of an anti-freezing agent; 5 to 20 parts of styrene-acrylic emulsion; 5 to 20 parts of silicone acrylic emulsion; 20 to 40 parts of heavy calcium carbonate; 20 to 40 parts of quartz sand; 0.1 to 2 parts of a thickening agent; and 1-5 parts of a curing agent. Through improvement and proportion adjustment of related raw materials, the problems of poor adhesion, poor water resistance, long construction period and the like of the two-component interface leveling material are obviously improved, and the two-component interface leveling material has outstanding advantages and is suitable for industrial popularization.
本发明公开了一种用于瓷砖翻新的高附着力双组份界面找平材料制备方法。原料包括去离子水10‑30份;纤维素0.1‑1份;膨润土0.1‑1份;分散剂0.1‑1份;消泡剂0.1‑1份;防腐剂0.1‑1份;成膜助剂0.1‑2份;pH调节剂0.1‑1份;防冻剂0.1‑2份;苯丙乳液5‑20份;硅丙乳液5‑20份;重质碳酸钙20‑40份;石英砂20‑40份;增稠剂0.1‑2份;固化剂1‑5份。通过相关原料的改进和比例调整对双组份界面找平材料的附着力差、耐水性差、施工周期长等问题具有明显的提升效果,优点突出,适合应用于工业推广。
Preparation method of high-adhesion two-component interface leveling material for tile renovation
The invention discloses a preparation method of a high-adhesion two-component interface leveling material for tile renovation. The raw materials comprise 10-30 parts of deionized water; 0.1 to 1 part of cellulose; 0.1 to 1 part of bentonite; 0.1-1 part of a dispersant; 0.1 to 1 part of a defoaming agent; 0.1-1 part of a preservative; 0.1-2 parts of a coalescing agent; 0.1 to 1 part of a pH regulator; 0.1-2 parts of an anti-freezing agent; 5 to 20 parts of styrene-acrylic emulsion; 5 to 20 parts of silicone acrylic emulsion; 20 to 40 parts of heavy calcium carbonate; 20 to 40 parts of quartz sand; 0.1 to 2 parts of a thickening agent; and 1-5 parts of a curing agent. Through improvement and proportion adjustment of related raw materials, the problems of poor adhesion, poor water resistance, long construction period and the like of the two-component interface leveling material are obviously improved, and the two-component interface leveling material has outstanding advantages and is suitable for industrial popularization.
本发明公开了一种用于瓷砖翻新的高附着力双组份界面找平材料制备方法。原料包括去离子水10‑30份;纤维素0.1‑1份;膨润土0.1‑1份;分散剂0.1‑1份;消泡剂0.1‑1份;防腐剂0.1‑1份;成膜助剂0.1‑2份;pH调节剂0.1‑1份;防冻剂0.1‑2份;苯丙乳液5‑20份;硅丙乳液5‑20份;重质碳酸钙20‑40份;石英砂20‑40份;增稠剂0.1‑2份;固化剂1‑5份。通过相关原料的改进和比例调整对双组份界面找平材料的附着力差、耐水性差、施工周期长等问题具有明显的提升效果,优点突出,适合应用于工业推广。
Preparation method of high-adhesion two-component interface leveling material for tile renovation
一种用于瓷砖翻新的高附着力双组份界面找平材料制备方法
SHI FENGLIANG (author) / LIANG BIN (author) / CHE BOYI (author) / PANG YUTING (author)