Geopolymer grouting material with enhanced electromagnetic performance and preparation method thereof
The invention provides a geopolymer grouting material with enhanced electromagnetic performance and a preparation method thereof, and belongs to the technical field of grouting materials, the geopolymer grouting material is composed of water and mixed slurry, the mass ratio of the water to the mixed slurry is 0.33-0.5, the mixed slurry is composed of a geopolymer grouting material, ferroferric oxide powder and a low-viscosity thickening agent, the mass ratio of the ferroferric oxide powder to the mixed slurry is 0.05-0.1, and the low-viscosity thickening agent is a mixture of the geopolymer grouting material, the ferroferric oxide powder and the low-viscosity thickening agent. The mass ratio of the low-viscosity thickening agent to the mixed slurry is 0.0001 to 0.0005. The development performance of the grouting material can be improved, engineers can conveniently and nondestructively detect the distribution condition of slurry through electronic scanning imaging equipment, the development performance of the grouting material can be improved, and the grouting effect can be nondestructively evaluated in cooperation with the electronic scanning imaging equipment.
本发明提供增强电磁性能的地聚合物注浆材料及其制备方法,属于注浆材料技术领域,由水和混合浆料组成,水:混合浆料的质量比为0.33~0.5,混合浆料由地聚合注浆材料、四氧化三铁粉和低粘度增稠剂组成,四氧化三铁粉:混合浆料的质量比为0.05~0.1,低粘度增稠剂:混合浆料的质量比为0.0001~0.0005。本发明可提高注浆材料的显影性能,便于工程人员通过电子扫描成像设备无损检测浆液的分布情况,可提高注浆材料的显影性能,配合电子扫描成像设备,可无损评价注浆效果。
Geopolymer grouting material with enhanced electromagnetic performance and preparation method thereof
The invention provides a geopolymer grouting material with enhanced electromagnetic performance and a preparation method thereof, and belongs to the technical field of grouting materials, the geopolymer grouting material is composed of water and mixed slurry, the mass ratio of the water to the mixed slurry is 0.33-0.5, the mixed slurry is composed of a geopolymer grouting material, ferroferric oxide powder and a low-viscosity thickening agent, the mass ratio of the ferroferric oxide powder to the mixed slurry is 0.05-0.1, and the low-viscosity thickening agent is a mixture of the geopolymer grouting material, the ferroferric oxide powder and the low-viscosity thickening agent. The mass ratio of the low-viscosity thickening agent to the mixed slurry is 0.0001 to 0.0005. The development performance of the grouting material can be improved, engineers can conveniently and nondestructively detect the distribution condition of slurry through electronic scanning imaging equipment, the development performance of the grouting material can be improved, and the grouting effect can be nondestructively evaluated in cooperation with the electronic scanning imaging equipment.
本发明提供增强电磁性能的地聚合物注浆材料及其制备方法,属于注浆材料技术领域,由水和混合浆料组成,水:混合浆料的质量比为0.33~0.5,混合浆料由地聚合注浆材料、四氧化三铁粉和低粘度增稠剂组成,四氧化三铁粉:混合浆料的质量比为0.05~0.1,低粘度增稠剂:混合浆料的质量比为0.0001~0.0005。本发明可提高注浆材料的显影性能,便于工程人员通过电子扫描成像设备无损检测浆液的分布情况,可提高注浆材料的显影性能,配合电子扫描成像设备,可无损评价注浆效果。
Geopolymer grouting material with enhanced electromagnetic performance and preparation method thereof
增强电磁性能的地聚合物注浆材料及其制备方法
CHEN DEQIANG (author) / LU CHANGHENG (author) / LUO JUNHUI (author) / MO PENG (author) / CHANG ZHENCHAO (author) / PAN ZHU (author)
2024-09-10
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Developing-enhanced geopolymer grouting material and preparation method thereof
European Patent Office | 2024
|Geopolymer grouting material and preparation method thereof
European Patent Office | 2023
|Geopolymer grouting material and preparation method thereof
European Patent Office | 2024
|High-performance geopolymer grouting material and preparation method thereof
European Patent Office | 2022
|Geopolymer cement grouting material and preparation method thereof
European Patent Office | 2023
|