Acid and alkali resistant ceramic and preparation process thereof
The acid and alkali resistant ceramic comprises the following components in parts by weight: 30-40 parts of kaolin, 20-30 parts of sodium tripolyphosphate, 20-30 parts of potassium feldspar, 8-10 parts of borax, 10-20 parts of magnesium oxide, 5-8 parts of zinc oxide, 5-8 parts of calcined talc and 8-10 parts of iron phosphate. According to the acid and alkali resistant ceramic and the preparation process thereof disclosed by the invention, the prepared ceramic artware has excellent mechanical property and acid and alkali resistance.
本发明一种耐酸碱的陶瓷,包括以下重量份的组分:高岭土30‑40份、三聚磷酸钠20‑30份、钾长石20‑30份、硼砂8‑10份、氧化镁10‑20份、氧化锌5‑8份、烧滑石5‑8份和磷酸铁8‑10份。本发明一种耐酸碱的陶瓷及其制备工艺,制得的陶瓷工艺品具有优异的机械性能和耐酸碱性能。
Acid and alkali resistant ceramic and preparation process thereof
The acid and alkali resistant ceramic comprises the following components in parts by weight: 30-40 parts of kaolin, 20-30 parts of sodium tripolyphosphate, 20-30 parts of potassium feldspar, 8-10 parts of borax, 10-20 parts of magnesium oxide, 5-8 parts of zinc oxide, 5-8 parts of calcined talc and 8-10 parts of iron phosphate. According to the acid and alkali resistant ceramic and the preparation process thereof disclosed by the invention, the prepared ceramic artware has excellent mechanical property and acid and alkali resistance.
本发明一种耐酸碱的陶瓷,包括以下重量份的组分:高岭土30‑40份、三聚磷酸钠20‑30份、钾长石20‑30份、硼砂8‑10份、氧化镁10‑20份、氧化锌5‑8份、烧滑石5‑8份和磷酸铁8‑10份。本发明一种耐酸碱的陶瓷及其制备工艺,制得的陶瓷工艺品具有优异的机械性能和耐酸碱性能。
Acid and alkali resistant ceramic and preparation process thereof
一种耐酸碱的陶瓷及其制备工艺
WEI LIANJIN (author) / LIN LIRONG (author) / WEI JUNFENG (author)
2024-10-15
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Alkali resistant ceramic coating material and preparation method thereof
European Patent Office | 2015
|Novel acid-resistant alkali-resistant carbon brick and preparation method thereof
European Patent Office | 2021
|European Patent Office | 2021
|