A platform for research: civil engineering, architecture and urbanism
Green repair construction method for urban ceramic tile facade
The invention relates to a green repair construction method for an urban ceramic tile facade, which comprises the following steps: firstly, cleaning an existing building facade, repairing hollow and cracked areas of ceramic tiles, and then leveling; then the outer surface of the wall body is filled with polymer cement mortar for leveling; the cement-based exterior wall putty is filled twice, a quick-drying agent is added into the putty to accelerate drying and forming of the putty, and then the putty is polished to be smooth; then, the outer surface of the putty is coated with base layer reinforced seal primer in a roller coating mode; the outer surface of the seal primer is coated with waterproof and decorative integrated paint twice in a roller coating mode; and the waterproof and decorative integrated coating continues to be coated with finishing paint in a roller coating mode, and wall repairing is completed. According to the method, the construction period can be shortened, large construction transformation on the outer wall surface structure of the existing building is avoided, cost reduction and efficiency improvement of the project are achieved, the service life of the building is prolonged, and use safety is guaranteed.
本发明涉及一种用于城市瓷砖外立面绿色修复施工方法,先清理既有建筑外立面,修补瓷砖空鼓、开裂区域后找平;然后再墙体外表面满批聚合物水泥砂浆找平;再满批水泥基外墙腻子两遍,腻子中加入快干剂加速腻子干燥成型,然后对腻子进行打磨平整;然后再在腻子外表面辊涂基层加固的封闭底漆;在封闭底漆外表面辊涂防水装饰一体化涂料两遍;在防水装饰一体化涂料外继续辊涂罩光面漆,完成墙体修复。本发明可缩短施工工期,避免了对既有建筑外墙面构造进行大的施工改造,实现工程降本增效,提高了建筑使用寿命和保障使用安全。
Green repair construction method for urban ceramic tile facade
The invention relates to a green repair construction method for an urban ceramic tile facade, which comprises the following steps: firstly, cleaning an existing building facade, repairing hollow and cracked areas of ceramic tiles, and then leveling; then the outer surface of the wall body is filled with polymer cement mortar for leveling; the cement-based exterior wall putty is filled twice, a quick-drying agent is added into the putty to accelerate drying and forming of the putty, and then the putty is polished to be smooth; then, the outer surface of the putty is coated with base layer reinforced seal primer in a roller coating mode; the outer surface of the seal primer is coated with waterproof and decorative integrated paint twice in a roller coating mode; and the waterproof and decorative integrated coating continues to be coated with finishing paint in a roller coating mode, and wall repairing is completed. According to the method, the construction period can be shortened, large construction transformation on the outer wall surface structure of the existing building is avoided, cost reduction and efficiency improvement of the project are achieved, the service life of the building is prolonged, and use safety is guaranteed.
本发明涉及一种用于城市瓷砖外立面绿色修复施工方法,先清理既有建筑外立面,修补瓷砖空鼓、开裂区域后找平;然后再墙体外表面满批聚合物水泥砂浆找平;再满批水泥基外墙腻子两遍,腻子中加入快干剂加速腻子干燥成型,然后对腻子进行打磨平整;然后再在腻子外表面辊涂基层加固的封闭底漆;在封闭底漆外表面辊涂防水装饰一体化涂料两遍;在防水装饰一体化涂料外继续辊涂罩光面漆,完成墙体修复。本发明可缩短施工工期,避免了对既有建筑外墙面构造进行大的施工改造,实现工程降本增效,提高了建筑使用寿命和保障使用安全。
Green repair construction method for urban ceramic tile facade
一种用于城市瓷砖外立面绿色修复施工方法
ZHANG MING (author) / ZHOU WENWU (author) / HU ZHIYUAN (author) / LI CHAO (author) / XIONG JUN (author) / ZHENG HAO (author) / SUN TAO (author) / ZENG XUGUANG (author) / PAN KANG (author)
2024-10-18
Patent
Electronic Resource
Chinese
Existing building ceramic tile facade transformed granitic plaster structure and construction method
European Patent Office | 2023
|Construction method for lossless repair of ceramic tile hollowing
European Patent Office | 2023
|Ceramic tile reverse construction formwork and ceramic tile reverse construction method
European Patent Office | 2015
|European Patent Office | 2024
|European Patent Office | 2020
|