A platform for research: civil engineering, architecture and urbanism
Green anti-cracking premixed concrete and preparation method thereof
The invention relates to the technical field of concrete, and particularly discloses green anti-cracking premixed concrete and a preparation method thereof. The green anti-cracking premixed concrete is prepared from the following raw materials in parts by weight: Portland cement, superfine fly ash, slag powder, river sand, broken stone, a polycarboxylic acid superplasticizer, waste concrete aggregate, ammonium polyphosphate modified wheat straw fibers, self-repairing microcapsules and water. The preparation method of the green anti-cracking premixed concrete comprises the following steps: S1, mixing and stirring the ammonium polyphosphate modified wheat straw fibers, the water and the self-repairing microcapsules to obtain a mixture A; s2, adding Portland cement, superfine fly ash, river sand, gravel, a polycarboxylic acid superplasticizer, waste concrete aggregate and slag powder into the mixture A, and stirring to obtain the green anti-cracking premixed concrete. The prepared green anti-cracking premixed concrete is excellent in anti-cracking performance, non-renewable mine resources are utilized, and the green anti-cracking premixed concrete is green and environmentally friendly.
本申请涉及混凝土技术领域,具体公开了一种绿色抗裂预拌混凝土及其制备方法。一种绿色抗裂预拌混凝土,包括如下重量份原料:硅酸盐水泥、超细粉煤灰、矿渣粉、河砂、碎石、聚羧酸高效减水剂、废旧混凝土集料、聚磷酸铵改性麦秸纤维、自修复微胶囊和水。一种绿色抗裂预拌混凝土的制备方法,包括以下步骤:S1、将聚磷酸铵改性麦秸纤维、水和自修复微胶囊混合搅拌,得到混合物A;S2、向混合物A中加入硅酸盐水泥、超细粉煤灰、河砂、碎石、聚羧酸高效减水剂、废旧混凝土集料、矿渣粉后,搅拌,制得所述绿色抗裂预拌混凝土。本申请制得的绿色抗裂预拌混凝土的抗裂性能优异,利用了不可再生的矿山资源,绿色环保。
Green anti-cracking premixed concrete and preparation method thereof
The invention relates to the technical field of concrete, and particularly discloses green anti-cracking premixed concrete and a preparation method thereof. The green anti-cracking premixed concrete is prepared from the following raw materials in parts by weight: Portland cement, superfine fly ash, slag powder, river sand, broken stone, a polycarboxylic acid superplasticizer, waste concrete aggregate, ammonium polyphosphate modified wheat straw fibers, self-repairing microcapsules and water. The preparation method of the green anti-cracking premixed concrete comprises the following steps: S1, mixing and stirring the ammonium polyphosphate modified wheat straw fibers, the water and the self-repairing microcapsules to obtain a mixture A; s2, adding Portland cement, superfine fly ash, river sand, gravel, a polycarboxylic acid superplasticizer, waste concrete aggregate and slag powder into the mixture A, and stirring to obtain the green anti-cracking premixed concrete. The prepared green anti-cracking premixed concrete is excellent in anti-cracking performance, non-renewable mine resources are utilized, and the green anti-cracking premixed concrete is green and environmentally friendly.
本申请涉及混凝土技术领域,具体公开了一种绿色抗裂预拌混凝土及其制备方法。一种绿色抗裂预拌混凝土,包括如下重量份原料:硅酸盐水泥、超细粉煤灰、矿渣粉、河砂、碎石、聚羧酸高效减水剂、废旧混凝土集料、聚磷酸铵改性麦秸纤维、自修复微胶囊和水。一种绿色抗裂预拌混凝土的制备方法,包括以下步骤:S1、将聚磷酸铵改性麦秸纤维、水和自修复微胶囊混合搅拌,得到混合物A;S2、向混合物A中加入硅酸盐水泥、超细粉煤灰、河砂、碎石、聚羧酸高效减水剂、废旧混凝土集料、矿渣粉后,搅拌,制得所述绿色抗裂预拌混凝土。本申请制得的绿色抗裂预拌混凝土的抗裂性能优异,利用了不可再生的矿山资源,绿色环保。
Green anti-cracking premixed concrete and preparation method thereof
一种绿色抗裂预拌混凝土及其制备方法
DU MINGSHENG (author) / LENKO (author) / DENG YAXI (author) / GONG XIAOSHUANG (author) / LIU YANG (author) / WANG CHUAN (author)
2024-11-19
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Environment-friendly anti-cracking premixed concrete and preparation method thereof
European Patent Office | 2023
|