A platform for research: civil engineering, architecture and urbanism
Self-healing polymer waterproof coiled material and preparation method thereof
The invention discloses a self-healing polymer waterproof coiled material and a preparation method thereof. The waterproof roll comprises a surface layer, a cement mortar layer containing a reinforcing layer, a butadiene rubber self-healing layer and a bottom layer, the surface layer is prepared from the following components in parts by weight: 30.0 to 50.0 parts of ethylene propylene diene monomer, 5.0 to 15.0 parts of SBS thermoplastic rubber, 5.0 to 15.0 parts of flame retardant, 5.0 to 10.0 parts of calcium carbonate master batch, 1.0 to 3.0 parts of root inhibitor, 1.0 to 3.0 parts of color master batch and 1.0 to 5.0 parts of antioxidant; the cement mortar layer and the bottom layer are prepared from the following components in parts by weight: 40.0 to 50.0 parts of 42.5 white cement, 10.0 to 20.0 parts of sodium silicate, 5.0 to 10.0 parts of bentonite, 5.0 to 15.0 parts of sodium polyacrylate, 10.0 to 15.0 parts of capillary crystalline master batch and 10.0 to 20.0 parts of quartz sand; the butadiene rubber self-healing layer is prepared from the following components in parts by weight: 30.0 to 50.0 parts of butadiene rubber, 10.0 to 15.0 parts of SBR (Styrene Butadiene Rubber), 10.0 to 20.0 parts of calcium carbonate filler, 5.0 to 10.0 parts of DIDP plasticizer, 1.0 to 5.0 parts of root inhibitor, 1.0 to 5.0 parts of vulcanizing agent and 10.0 to 20.0 parts of microcapsule vulcanized particles.
本发明公开了一种自愈型高分子防水卷材及其制备方法;该防水卷材包括面层、含有加强层的水泥胶砂层、顺丁橡胶自愈层、底层;面层按照重量份数包括30.0~50.0份三元乙丙橡胶、5.0~15.0份SBS热塑性橡胶、5.0~15.0份阻燃剂、5.0~10.0份碳酸钙母粒、1.0~3.0份阻根剂、1.0~3.0份色母和1.0~5.0份抗氧剂;水泥胶砂层以及底层按照重量份数包括40.0~50.0份42.5白水泥、10.0~20.0份硅酸钠、5.0~10.0份膨润土、5.0~15.0份聚丙烯酸钠、10.0~15.0份渗透结晶母料、10.0~20.0份石英砂;顺丁橡胶自愈层按照重量份数包括30.0~50.0份顺丁橡胶、10.0~15.0份SBR、10.0~20.0份碳酸钙填料、5.0~10.0份DIDP增塑剂、1.0~5.0份阻根剂、1.0~5.0份硫化剂、10.0~20.0份微胶囊硫化颗粒。
Self-healing polymer waterproof coiled material and preparation method thereof
The invention discloses a self-healing polymer waterproof coiled material and a preparation method thereof. The waterproof roll comprises a surface layer, a cement mortar layer containing a reinforcing layer, a butadiene rubber self-healing layer and a bottom layer, the surface layer is prepared from the following components in parts by weight: 30.0 to 50.0 parts of ethylene propylene diene monomer, 5.0 to 15.0 parts of SBS thermoplastic rubber, 5.0 to 15.0 parts of flame retardant, 5.0 to 10.0 parts of calcium carbonate master batch, 1.0 to 3.0 parts of root inhibitor, 1.0 to 3.0 parts of color master batch and 1.0 to 5.0 parts of antioxidant; the cement mortar layer and the bottom layer are prepared from the following components in parts by weight: 40.0 to 50.0 parts of 42.5 white cement, 10.0 to 20.0 parts of sodium silicate, 5.0 to 10.0 parts of bentonite, 5.0 to 15.0 parts of sodium polyacrylate, 10.0 to 15.0 parts of capillary crystalline master batch and 10.0 to 20.0 parts of quartz sand; the butadiene rubber self-healing layer is prepared from the following components in parts by weight: 30.0 to 50.0 parts of butadiene rubber, 10.0 to 15.0 parts of SBR (Styrene Butadiene Rubber), 10.0 to 20.0 parts of calcium carbonate filler, 5.0 to 10.0 parts of DIDP plasticizer, 1.0 to 5.0 parts of root inhibitor, 1.0 to 5.0 parts of vulcanizing agent and 10.0 to 20.0 parts of microcapsule vulcanized particles.
本发明公开了一种自愈型高分子防水卷材及其制备方法;该防水卷材包括面层、含有加强层的水泥胶砂层、顺丁橡胶自愈层、底层;面层按照重量份数包括30.0~50.0份三元乙丙橡胶、5.0~15.0份SBS热塑性橡胶、5.0~15.0份阻燃剂、5.0~10.0份碳酸钙母粒、1.0~3.0份阻根剂、1.0~3.0份色母和1.0~5.0份抗氧剂;水泥胶砂层以及底层按照重量份数包括40.0~50.0份42.5白水泥、10.0~20.0份硅酸钠、5.0~10.0份膨润土、5.0~15.0份聚丙烯酸钠、10.0~15.0份渗透结晶母料、10.0~20.0份石英砂;顺丁橡胶自愈层按照重量份数包括30.0~50.0份顺丁橡胶、10.0~15.0份SBR、10.0~20.0份碳酸钙填料、5.0~10.0份DIDP增塑剂、1.0~5.0份阻根剂、1.0~5.0份硫化剂、10.0~20.0份微胶囊硫化颗粒。
Self-healing polymer waterproof coiled material and preparation method thereof
一种自愈型高分子防水卷材及其制备方法
ZHU HUA (author) / GUO WEI (author) / ZHAO CHANGCAI (author) / LI DENGJUN (author) / HAO KUNBO (author)
2024-12-06
Patent
Electronic Resource
Chinese
IPC:
B32B
LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
,
Schichtkörper, d.h. aus Ebenen oder gewölbten Schichten, z.B. mit zell- oder wabenförmiger Form, aufgebaute Erzeugnisse
/
B29D
PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE
,
Herstellen besonderer Gegenstände aus Kunststoff oder aus Stoffen in plastischem Zustand
/
E02D
FOUNDATIONS
,
Gründungen
/
E04B
Allgemeine Baukonstruktionen
,
GENERAL BUILDING CONSTRUCTIONS
/
E04D
ROOF COVERINGS
,
Dacheindeckungen
Self-adhesive polymer waterproof coiled material and preparation method thereof
European Patent Office | 2024
|Root-puncture-resistant self-healing waterproof coiled material and preparation method thereof
European Patent Office | 2020
|European Patent Office | 2024
|Butyl rubber polymer self-adhesive waterproof coiled material and preparation method thereof
European Patent Office | 2024
|European Patent Office | 2024
|