The invention discloses a toilet crack sealing process using a multi-component sealing material, which comprises the following steps of: 1, cleaning dust, dirt and loose parts on the surface of a wall surface or a floor around a crack, and washing with clear water to ensure that the surface is dry and free of oil stain; 2, for a relatively wide crack, a filler can be firstly used for preliminary filling so as to reduce the width of the crack; 3, uniformly smearing the prepared multi-component high-performance resin alloy sealing material on the surface of the crack, and fully permeating and filling the crack by utilizing the fluidity of the material; 4, after the sealing material is cured, the crack sealing condition is checked in the curing process, and supplementary smearing is carried out when necessary; the invention has the following beneficial effects: the use of the multi-component high-performance resin alloy sealing material effectively prevents water vapor permeation and protects a building structure; the material combines rigidity and softness, is high in weather resistance and can keep a crack sealing effect for a long time.
本发明公开了一种使用多组分密封材料的厕所裂缝封闭工艺,包括如下步骤:步骤一:清理裂缝周围墙面或地板表面的粉尘、污垢及松散部分,并用清水冲洗干净,确保表面干燥无油污;步骤二:对于较宽的裂缝,可先用填充物进行初步填补,以减少裂缝宽度;步骤三:将配制好的多组分高性能树脂合金密封材料均匀涂抹在裂缝表面,利用材料的流动性充分渗透并填满裂缝;步骤四:等待密封材料固化,固化过程中检查裂缝封闭情况,必要时进行补充涂抹;本发明的有益效果是:多组分高性能树脂合金密封材料的使用有效阻止水汽渗透,保护建筑结构;材料刚柔结合,耐候性强,能够长期保持裂缝封闭效果。
Toilet crack sealing process using multi-component sealing material
The invention discloses a toilet crack sealing process using a multi-component sealing material, which comprises the following steps of: 1, cleaning dust, dirt and loose parts on the surface of a wall surface or a floor around a crack, and washing with clear water to ensure that the surface is dry and free of oil stain; 2, for a relatively wide crack, a filler can be firstly used for preliminary filling so as to reduce the width of the crack; 3, uniformly smearing the prepared multi-component high-performance resin alloy sealing material on the surface of the crack, and fully permeating and filling the crack by utilizing the fluidity of the material; 4, after the sealing material is cured, the crack sealing condition is checked in the curing process, and supplementary smearing is carried out when necessary; the invention has the following beneficial effects: the use of the multi-component high-performance resin alloy sealing material effectively prevents water vapor permeation and protects a building structure; the material combines rigidity and softness, is high in weather resistance and can keep a crack sealing effect for a long time.
本发明公开了一种使用多组分密封材料的厕所裂缝封闭工艺,包括如下步骤:步骤一:清理裂缝周围墙面或地板表面的粉尘、污垢及松散部分,并用清水冲洗干净,确保表面干燥无油污;步骤二:对于较宽的裂缝,可先用填充物进行初步填补,以减少裂缝宽度;步骤三:将配制好的多组分高性能树脂合金密封材料均匀涂抹在裂缝表面,利用材料的流动性充分渗透并填满裂缝;步骤四:等待密封材料固化,固化过程中检查裂缝封闭情况,必要时进行补充涂抹;本发明的有益效果是:多组分高性能树脂合金密封材料的使用有效阻止水汽渗透,保护建筑结构;材料刚柔结合,耐候性强,能够长期保持裂缝封闭效果。
Toilet crack sealing process using multi-component sealing material
一种使用多组分密封材料的厕所裂缝封闭工艺
LI JIANDA (author) / MA BAOLIANG (author) / LI QIAN (author)
2024-12-10
Patent
Electronic Resource
Chinese
IPC:
E04G
SCAFFOLDING
,
Baugerüste