METHOD AND APPARATUS FOR THE PREPARATION OF FINELY DIVIDED CALCIUM HYDROXIDE
Method for the preparation of finely divided calcium hydroxide, where calcium oxide is comminuted in an impact disintegrator into which in addition to the calcium hydroxide a small amount of water is led to wet the particles obtained and to bind the dust. The calcium oxide powder is led to a conveyor being in connection with the impact disintegrator and operating as a pre-quencher, to which conveyer water is added and where the material is subjected to a kneading effect. The material which is a mixture of calcium oxide and calcium hydroxide is led from the conveyor to a cistern operating as post-quencher, to which cistern the remaining portion of the total water amount required for quenching is added. The amount of water added to the impact disintegrator and to the pre-quencher is altogether 20 . . . 50% of the total amount of water required for quenching, preferably about 1/3 of the total amount of water required for quenching, and the amount of water added to the post-quencher is 80 . . . 50% of the total amount of water required for quenching, preferably about 2/3 of the total amount of water required for quenching.
METHOD AND APPARATUS FOR THE PREPARATION OF FINELY DIVIDED CALCIUM HYDROXIDE
Method for the preparation of finely divided calcium hydroxide, where calcium oxide is comminuted in an impact disintegrator into which in addition to the calcium hydroxide a small amount of water is led to wet the particles obtained and to bind the dust. The calcium oxide powder is led to a conveyor being in connection with the impact disintegrator and operating as a pre-quencher, to which conveyer water is added and where the material is subjected to a kneading effect. The material which is a mixture of calcium oxide and calcium hydroxide is led from the conveyor to a cistern operating as post-quencher, to which cistern the remaining portion of the total water amount required for quenching is added. The amount of water added to the impact disintegrator and to the pre-quencher is altogether 20 . . . 50% of the total amount of water required for quenching, preferably about 1/3 of the total amount of water required for quenching, and the amount of water added to the post-quencher is 80 . . . 50% of the total amount of water required for quenching, preferably about 2/3 of the total amount of water required for quenching.
METHOD AND APPARATUS FOR THE PREPARATION OF FINELY DIVIDED CALCIUM HYDROXIDE
VERFAHREN UND VORRICHTUNG ZUR HERSTELLUNG VON FEIN GETEILTEM CALCIUMHYDROXID
PROCÉDÉ ET APPAREIL POUR LA PRÉPARATION D'HYDROXYDE DE CALCIUM FINEMENT DIVISÉ
VIRTANEN PENTTI (author)
2016-05-25
Patent
Electronic Resource
English
IPC:
C01F
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS
,
Verbindungen der Metalle Beryllium, Magnesium, Aluminium, Calcium, Strontium, Barium, Radium, Thorium oder der Seltenen Erden
/
B02C
CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL
,
Brechen, Pulverisieren oder Zerkleinern allgemein
/
C04B
Kalk
,
LIME
METHOD TO ARTIFICIALLY AGGLOMERATE FINELY DIVIDED MATERIALS
European Patent Office | 2018
|Method to artificially agglomerate finely divided materials
European Patent Office | 2020
|METHOD TO ARTIFICIALLY AGGLOMERATE FINELY DIVIDED MATERIALS
European Patent Office | 2018
|METHOD TO ARTIFICIALLY AGGLOMERATE FINELY DIVIDED MATERIALS
European Patent Office | 2016
|EXPERIMENTAL STUDY HETEROGENEOUS POLYMER COMPOSITES WITH FINELY DIVIDED FILLER
DOAJ | 2015
|