BAUGRUPPE MIT ZWEI MITEINANDER GEFÜGTEN KERAMIKKÖRPERN, INSBESONDERE DRUCKMESSZELLE, UND VERFAHREN ZUM FÜGEN VON KERAMIKKÖRPERN MITTELS EINES AKTIVHARTLOTS
An assembly comprising: two ceramic bodies, which are joined by means of a joint of an active hard solder, or braze, wherein the active hard solder, or braze, has a continuous core volume, which is spaced, in each case, from the ceramic bodies by at least 1 μm, and an average composition CK with a liquidus temperature Tl(CK), wherein the composition CK has a coefficient of thermal expansion α(CK), wherein α(CK)=m·α(K), wherein m≤1.5, especially m≤1.3 and preferably m≤1.2, wherein α(K) is the average coefficient of thermal expansion of the ceramic material of the ceramic bodies, wherein the joint has boundary layers, which border on the ceramic body, wherein at least one of the boundary layers, which lies outside of the core volume, has an average composition CB with a liquidus temperature Tl(CB), which lies not less than 50 K, preferably not less than 100 K, and especially preferably not less than 200 K, under the liquidus temperature Tl(CK) of the average composition CK of the core volume.
BAUGRUPPE MIT ZWEI MITEINANDER GEFÜGTEN KERAMIKKÖRPERN, INSBESONDERE DRUCKMESSZELLE, UND VERFAHREN ZUM FÜGEN VON KERAMIKKÖRPERN MITTELS EINES AKTIVHARTLOTS
An assembly comprising: two ceramic bodies, which are joined by means of a joint of an active hard solder, or braze, wherein the active hard solder, or braze, has a continuous core volume, which is spaced, in each case, from the ceramic bodies by at least 1 μm, and an average composition CK with a liquidus temperature Tl(CK), wherein the composition CK has a coefficient of thermal expansion α(CK), wherein α(CK)=m·α(K), wherein m≤1.5, especially m≤1.3 and preferably m≤1.2, wherein α(K) is the average coefficient of thermal expansion of the ceramic material of the ceramic bodies, wherein the joint has boundary layers, which border on the ceramic body, wherein at least one of the boundary layers, which lies outside of the core volume, has an average composition CB with a liquidus temperature Tl(CB), which lies not less than 50 K, preferably not less than 100 K, and especially preferably not less than 200 K, under the liquidus temperature Tl(CK) of the average composition CK of the core volume.
BAUGRUPPE MIT ZWEI MITEINANDER GEFÜGTEN KERAMIKKÖRPERN, INSBESONDERE DRUCKMESSZELLE, UND VERFAHREN ZUM FÜGEN VON KERAMIKKÖRPERN MITTELS EINES AKTIVHARTLOTS
ASSEMBLY COMPRISING TWO CERAMIC BODIES JOINED TO ONE ANOTHER, IN PARTICULAR A PRESSURE MEASURING CELL, AND METHOD FOR JOINING CERAMIC BODIES BY MEANS OF AN ACTIVE HARD SOLDER
SOUS-ENSEMBLE COMPRENANT DEUX CORPS EN CÉRAMIQUE ASSEMBLÉS, EN PARTICULIER UNE CELLULE DYNAMOMÉTRIQUE, ET PROCÉDÉ D'ASSEMBLAGE DE CORPS EN CÉRAMIQUE AU MOYEN D'UN MÉTAL D'APPORT ACTIF POUR BRASAGE FORT
ROSSBERG ANDREAS (author) / SCHMIDT ELKE (author) / RETTENMAYR MARKUS (author) / SIEGMUND PETER (author)
2022-04-27
Patent
Electronic Resource
German
IPC:
C04B
Kalk
,
LIME
/
B23K
Löten
,
SOLDERING OR UNSOLDERING
/
C22C
Legierungen
,
ALLOYS
/
G01L
Messen von Kraft, mechanischer Spannung, Drehmoment, Arbeit, mechanischer Leistung, mechanischem Wirkungsgrad oder des Drucks von Fluiden
,
MEASURING FORCE, STRESS, TORQUE, WORK, MECHANICAL POWER, MECHANICAL EFFICIENCY, OR FLUID PRESSURE
European Patent Office | 2016
|European Patent Office | 2016
|Taminabrücke Pfäfers (SG) Zwei Seiten eines Bergtals sind miteinander verbunden
British Library Online Contents | 2017